#1 User is offline   Min Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 33
  • Joined: 31-March 10
  • LocationCanada

Posted 15 February 2013 - 11:31 AM

Does anyone have a method to check for crazing with dark glazes? My normal method for craze testing is to heat a glazed test pot in the oven @ 325 for 30 minutes then plunge the pot into room temp water, then repeat procedure twice, each time increasing the oven temp by 5 degrees. Then I rub sumi ink onto the pot, leave it sit for a few minutes, rinse and check for crazing. Works for clear, whites and most glazes but obviously not for black or very dark brown etc. I tried floating a solution of isopropanol and nepsy on a flat test piece, logic being the alcohol would evaporate leaving the nepsy in the crazing if there was any. Results were messy and not that conclusive. Any suggestions?
0

#2 User is offline   Diane Puckett Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 173
  • Joined: 18-July 11
  • LocationAsheville, NC

Posted 16 February 2013 - 03:05 PM

What about white ink? Dick Blick sells it online.
Diane Puckett
Dry Ridge Pottery
0

#3 User is offline   Min Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 33
  • Joined: 31-March 10
  • LocationCanada

Posted 16 February 2013 - 06:38 PM

Thanks for the idea Diane, I'll give it a try with a high expansion glaze that I know would craze on my clay to try it and see.




View PostDiane Puckett, on 16 February 2013 - 12:05 PM, said:

What about white ink? Dick Blick sells it online.

0

#4 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 16 February 2013 - 09:27 PM

An LED flashlight may show crazing.