wax on kiln shelves

#1 User is offline   minspargal Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 56
  • Joined: 21-February 11
  • LocationPort Aransas, Tx

Posted 14 February 2013 - 05:56 AM

I spilled a container of wax resit on a brand new shelf. I scraped off all i could. Can i just bisque it by itself to burn off the wax?
0

#2 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 14 February 2013 - 08:05 AM

That will work just fine.
0

#3 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 14 February 2013 - 08:23 AM

Be sure to vent well.
INRI
0

#4 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 695
  • Joined: 07-December 11
  • LocationCanada

Posted 14 February 2013 - 09:49 AM

View Postminspargal, on 14 February 2013 - 04:56 AM, said:

I spilled a container of wax resit on a brand new shelf. I scraped off all i could. Can i just bisque it by itself to burn off the wax?


Could have been worse. Could have been a jar of gold lustre. Or maybe a bottle of cobalt carb. mixed as a slip.Fire up your bisque kiln, and make sure you are out of the room while it is firing.
TJR.:Dsrc="http://ceramicartsdaily.org/community/public/style_emoticons/default/biggrin.gif">
I always try these emoticums. I left you a smiley face. Picture it in your mind.We all make mistakes.
0

#5 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,419
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 14 February 2013 - 09:54 AM

good lesson in disappearing wax! No residue just lots of stinky carbon.

Marcia
Marcia Selsor
0

#6 User is offline   minspargal Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 56
  • Joined: 21-February 11
  • LocationPort Aransas, Tx

Posted 14 February 2013 - 10:17 AM

I have a vent system, i wonder what would be the lowest temp cone wise to burn this off? And yes a bottle of gold luster would have been worse in $$$ and smell.
0

#7 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,191
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 14 February 2013 - 11:33 AM

I would take it up to 1000F to be safe. Just fire it up fast. I generally notice wax burning smell at around 600 degrees.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users