: Underfire Condition -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Underfire Condition Rate Topic: -----

#1 User is offline   Mark McCombs Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 111
  • Joined: 13-August 12
  • LocationSW Washington

Posted 11 February 2013 - 11:36 AM

I need to re-fire a ^6 ox load and get to the proper temp. Programming error on my part.

Do I use the same cones that have seen the same heat work as the ware, or do I use a new set of cones?



Thanks.
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt
0

#2 User is offline   Arnold Howard Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 185
  • Joined: 26-May 10
  • LocationMesquite, Texas USA

Posted 11 February 2013 - 12:29 PM

View PostMark McCombs, on 11 February 2013 - 10:36 AM, said:

I need to re-fire a ^6 ox load and get to the proper temp. Programming error on my part.

Do I use the same cones that have seen the same heat work as the ware, or do I use a new set of cones?


Several years ago I refired cones and compared them with new cones. I wrote, "If the kiln shuts off within 100F / 56C of the cone’s maturity, and the kiln temperature drops 50F / 28C, do not reuse the cones. They will not bend properly. This is because a hard shell will form on the cones. If you are not sure how hot the kiln fired before it turned off, use fresh cones in the next firing."

The link shows a photo of the refired cones and the new ones.

http://www.paragonwe...ter.cfm?PID=361

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com
0

#3 User is offline   Mark McCombs Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 111
  • Joined: 13-August 12
  • LocationSW Washington

Posted 11 February 2013 - 12:31 PM

Thank you.



I do know that the temp hit 1945F.
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt
0

#4 User is offline   Mark McCombs Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 111
  • Joined: 13-August 12
  • LocationSW Washington

Posted 11 February 2013 - 12:40 PM

I now have both new and slightly used cones in the kiln.



Thank you, Arnold.
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic