Can someone advise when is the best stage of drying to carve porcelain? I have just started throwing and handbuilding with porcelain and not sure whether it is leather hard or dry.

Thanks Annie
0

#2 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 06 February 2013 - 06:48 AM

The most important thing is to limit the amount of dust that you will create.
You have to determine the best texture for your carving.
Try carving at different 'water content textures' and see what feels best to you. Get a spray bottle just incase you may need to add a little water.
INRI
0

#3 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,440
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 06 February 2013 - 07:17 AM

I start carving after trimming. Leather hard. I sometimes squirt the surface for a gentle moistening.
Smoothing the edges with a damp chamois is an easy clean up rather than sanding when dry.

Marcia
Marcia Selsor
0

#4 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,367
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 06 February 2013 - 12:01 PM

The answer lies with what you want your carving to look like as each stage will give you a different look. As your porcelain dries your lines will go from soft and flowing to sharp and precise. Also, every type of porcelain will react a bit differently at each stage with some being more forgiving than others.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#5 User is offline   anniec9 Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 18
  • Joined: 04-June 12

Posted 07 February 2013 - 09:54 PM

Thank you everyone for your help. I can see I will need to try at different stages to find the result I want.