Posted 05 February 2013 - 12:20 PM

I am making a bowl and want to apply glaze at cone 10 only on the inner surface, then refire it at cone 5 with underglaze for vibrant colors. Is this even possible? Will the inner glaze be damaged? Any help is welcomed!
0

#2 User is online   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,446
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 05 February 2013 - 01:46 PM

Yes it is possible but be careful that you don't shock the matured/vitrified clay on the second glaze firing. you may have a tricky time getting the ^5 glaze to stick after the ^10 firing but it is possible. You can get brighter colors at ^10 if you use encapsulated stains. That could save you the hassle of 2 glaze firings and struggling with glaze application on a vitrified body.



Marcia
Marcia Selsor
0

#3 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,204
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 05 February 2013 - 02:14 PM

There's also a decent chance that the cone 10 glaze will change in the cone 5 firing- color shift, glossiness change, etc. Test it first.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#4 User is offline   druttaro Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 05-February 13

Posted 05 February 2013 - 02:33 PM

Thanks for the replies.

I do have a test piece drying but wanted to see if it was even possible. I am not to concerned with color change to the ^10 glaze but don't want it to change texture.

I am doing sugar skulls so will be happiest with good color on the outside.

Attached File(s)

  • Attached File  bowl.png (2.6MB)
    Number of downloads: 60

0

#5 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 05 February 2013 - 03:18 PM

Something to think about . . . why not use a cone 5/6 claybody, glaze fire to cone 6 and apply the underglazes for the same fire? I am assuming your underglazes are for the sprigs attached to the outside of the bowl. Save yourself time and the cost of the extra firing.


0

#6 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,366
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 05 February 2013 - 04:25 PM

I am a cone guy-and most glazes will change somewhat when fired again to lower temp. That is a shiny glaze can become matt etc.
I am with Marcia on the cone 6 all the way body-
Testing is the only way to know any of this as you are in unchartered territory.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#7 User is offline   druttaro Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 05-February 13

Posted 06 February 2013 - 07:11 PM

I am taking a class at my university and have to use the clay available.
0

#8 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 06 February 2013 - 09:57 PM

Why must you do this, are these the only glazes available to you?



INRI
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users