preparing raw majolica glaze for surface decoration.

#1 User is offline   Babs Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 5
  • Joined: 25-January 13

Posted 25 January 2013 - 07:52 PM

Hi I am looking for a way to make my raw majolica glaze "harder" so that I can ddo more painterly desings on my ware. Mybrush tends to clog up with the glaze powder and so the lines are interrupted.
Hope somepone can help. I think I readd somewhere that you can spray something onto the glaze.Does any one have any hints.
Babs
0

#2 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 25 January 2013 - 10:31 PM

Here is a link to a handout from Linda Arbuckle on majolica, including hardening the base glaze . . . http://lindaarbuckle...handout2007.pdf
0

#3 User is offline   SShirley Icon

  • Cow Creek Pottery
  • PipPipPip
  • Group: Members
  • Posts: 189
  • Joined: 31-March 10
  • LocationPittsburg, Kansas

Posted 25 January 2013 - 11:13 PM

I have added molasses to majolica to harden it, and it smells nice too, but molds after a while.
0

#4 User is offline   minspargal Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 56
  • Joined: 21-February 11
  • LocationPort Aransas, Tx

Posted 26 January 2013 - 08:56 AM

I use spray starch on mine and paint like you are using watercolors.
0

#5 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 134
  • Joined: 20-May 12
  • LocationColorado

Posted 26 January 2013 - 09:55 AM

You can fire your ware to cone 018 after you glaze and sand the peice. This cinters the glaze paricles making it a bit more sturdy.





Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#6 User is offline   Babs Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 5
  • Joined: 25-January 13

Posted 26 January 2013 - 08:01 PM

Thanks everyone for your practical suggestions as I was dreading having to rejig my glaze recipe for this order, someone wanting handwritten text on some posts..
Babs
0

#7 User is offline   minspargal Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 56
  • Joined: 21-February 11
  • LocationPort Aransas, Tx

Posted 27 January 2013 - 09:27 AM

It helps to have the right type of brushes, too. Those thin very long haired liner brushes are great for text. Good luck!
0

#8 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,431
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 28 January 2013 - 12:19 PM

As previously mentioned you can spray it with spray starch or cheap hair spray. You can also add a little liquid starch into the glaze batch.
I think it is mentioned in Arbuckle's information.

Marcia
Marcia Selsor
0

#9 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 171
  • Joined: 08-February 12
  • LocationCalifornia

Posted 07 February 2013 - 12:52 PM

add CMC to your base glaze. commercial glazes contain a good amount of this in their recipe. it forms sort of a "candy coating" and stiffens up the unfired glaze, which will be more resistant to your detail brush. start with around 1% or keep a thick solution of it in a jug to add to your glazes, underglazes, and stains/washes.
0

#10 User is offline   Babs Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 5
  • Joined: 25-January 13

Posted 07 February 2013 - 09:06 PM

Thanks everyone, about to bisque the 'thing' and then pending survival, will glaze and decorate using your suggestions.
Thanks again.
Babs