Color Active Slip Using a lower cone slip.

#1 User is offline   yedrow Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 362
  • Joined: 06-February 12

Posted 21 January 2013 - 05:31 AM

I can't find any recipes for a cone 6 "color active," or fluxing slip. I'm really not sure what designates a slip as such, beyond the presence of more than normal percentages of flux(s). If I were to use a lower cone slip would it act like a color active slip?

Joel.
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,360
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 21 January 2013 - 01:32 PM

Colored slips for me are slip (made from whatever clay body I choose) with added colorants to get a colored slip.-Fluxing slips for me are slips with fluxes added or lower cone clays which flux at high temps-I never have used ether .
I have colored porc or stoneware to make colored slips-most of this has been salt fired.
I have no idea what a color active slip is?
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 136
  • Joined: 20-May 12
  • LocationColorado

Posted 21 January 2013 - 11:05 PM

I'm not totally sure, but i think if you added like one part frit 3124 to one part colored slip you'd have a color active slip.



Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#4 User is offline   yedrow Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 362
  • Joined: 06-February 12

Posted 21 January 2013 - 11:18 PM

View PostIforgot, on 21 January 2013 - 11:05 PM, said:

I'm not totally sure, but i think if you added like one part frit 3124 to one part colored slip you'd have a color active slip.



Darrel


Thanks Darrel, I'll try a test using 3124.

I'm not sure either Mark. For now it is a pottery term that is awaiting concise definition. Like so many other pottery terms, it may never find one, heh.

Joel.