#1 User is offline   Ginny C Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 47
  • Joined: 02-April 10
  • LocationFort Wayne, IN

Posted 19 January 2013 - 05:29 PM

If I succeed in uploading a photo, you'll see a crack where the handle attaches to a bone dry mug. The crack doesn't go all the way around, just across the top half. (I know it's because the cup was a bit too dry when I attached the handle, but I'd like to save it if possible! I dried it upside down so the weight wouldn't pull the handle off, but this crack appeared anyway.)
Should I brush in some paper clay slip? I have some that's pretty thick and stiff, so it wouldn't add much moisture.

If I don't, is the crack likely to get worse in the bisque firing??

Laguna B-mix cone 5. Will bisque to 06 and then glaze fire to cone 6.

Ginny C
Attached File  IMG_6643.jpg (994.84K)
Number of downloads: 103
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,356
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 19 January 2013 - 05:32 PM

Best fixed before bisquing-Tool in some slip and then after drying rub it out with a sharp tool. Then fire.If its still cracked after firing try some bisque fix by amaco.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,365
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 19 January 2013 - 05:45 PM

Just be very aware of that mug if you try to use it for hot beverages as that might always be a weak spot. Cracks never really go away. : - )
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#4 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,356
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 19 January 2013 - 09:36 PM

You can use a kiln cement on the crack after bisquing to get the strength back.Hi fire mender is one I like as you mix your clay body with it and then mix it so repairs are a good match.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#5 User is online   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 945
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 19 January 2013 - 10:27 PM

Toss it or you'll spend more time "fixing" it (and not being sure it's really fixed) than it would take to make a replacement.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#6 User is offline   JessicaGrayCeramics Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 11
  • Joined: 06-January 13
  • LocationFeltwell, United Kingdom

Posted 20 January 2013 - 05:43 AM

View PostOffCenter, on 20 January 2013 - 03:27 AM, said:

Toss it or you'll spend more time "fixing" it (and not being sure it's really fixed) than it would take to make a replacement.


I'm with Jim. At least at this point, you can still reuse the clay.
Jessica Gray, MFA
www.JessicaGrayCeramics.com
0

#7 User is offline   emptynester Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 24-December 12

Posted 20 January 2013 - 10:00 AM

I can see why you would like to save it. It has nice details. That being said, I would reclaim the clay now. I haven't had great results with repairs. The glaze seems to high light the repaired area.
0

#8 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 134
  • Joined: 20-May 12
  • LocationColorado

Posted 20 January 2013 - 12:57 PM

I'd shove some sodium sillicate into the crack with a hard brush before bisque.



Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit