: Steven Hill Glaze -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Steven Hill Glaze

#1 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 134
  • Joined: 20-May 12
  • LocationColorado

Posted 18 January 2013 - 10:32 PM

Hey World,

I was reading this awesome article by steven hill about reduction look glazes at cone 6 in an electric kiln, but the firing schedule was for a kiln with a computer, and i have a manual kiln, how should i do this, i attached the recipie for the glaze and the firing schedule, thanks!


Darrel

Attached File(s)


Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#2 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 134
  • Joined: 20-May 12
  • LocationColorado

Posted 18 January 2013 - 11:05 PM

oops, here is the firing schedule.

Attached File(s)


Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#3 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,356
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 19 January 2013 - 01:34 AM

Its going to be a crap shoot at best but you WILL need a digital pyrometer and lots of time to babysit the kiln with a clock and a clear head. With your manual switch kiln try and recreate this schedule. every time will be an gamble on results.
I suggest trying your own glazes and schedules with what you have. You may find the results could be great and they will be yours.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#4 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,191
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 19 January 2013 - 09:46 AM

View PostMark C., on 19 January 2013 - 12:34 AM, said:

I suggest trying your own glazes and schedules with what you have. You may find the results could be great and they will be yours.
Mark


Bingo. Every show I go to has at least one potter making Steven Hill pots. While they are beautiful, they are just copies, and show very little creativity and certainly don't represent the personality of the potter. So if you do decide to use his glazes, figure out a way to make them uniquely yours.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#5 User is offline   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 949
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 19 January 2013 - 09:58 AM

Before you go to all the trouble of doing a controlled cool down in a manual kiln, try just firing the Hill glazes one cone higher. I think you'll like the results.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#6 User is online   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,488
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 19 January 2013 - 01:06 PM

Instead of shutting the kiln completely off when the firing cone is down, turn all the elements to low for a couple of hours. See what you get. Likely you will be happy.

best,

.............john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art