Make your own bats Rate Topic: -----

#21 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 25 January 2013 - 05:51 PM

View PostWahine, on 22 January 2013 - 01:56 PM, said:

Pres,

I was just planning to make some plaster bats. Why did you make a double groove for the foot ring? In my mind I'm thinking a single groove. Could you please elaborate? Also, did you cut the rings with a loop tool? Thanks,

-chantay



A double ring foot on a plate helps prevent sagging in the middle . . . which, on a large plate, would be less supported. Some potters also put a wad, perhaps with their chop mark or stamp, in the center of the plate to provide support against slumping during glaze firing.