Very thick glace Takuro Kuwata's glace

#1 User is offline   claclana Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 55
  • Joined: 17-April 11
  • LocationBuffalo, NY

Posted 08 January 2013 - 12:17 AM

how this awesome superthick glaze is achieved?
specially that gorgeous yellow bowl with white glaze big drips...
from the master Takuro Kuwata

Thank you for your help!
0

#2 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 739
  • Joined: 07-December 11
  • LocationCanada

Posted 08 January 2013 - 08:48 AM

Clayclana;
Looks like he's got one glaze underneath. The red in some cases, and blue in others. YoU apply that glaze to the bisque pot, let it dry, then apply a really thicK white that tends to crawl, like a Shino glaze. It helps if the first glaze is slightly shiny, then the top glaze pulls off.
Don't forget to make test tiles, and test,test,test.
TJR
0

#3 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,399
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 08 January 2013 - 02:51 PM

Thanks for sharing this site.
Some look like thick dry lichen glazes which you can find recipes for ... but I have no idea how he does the thick, gluey looking ones.
I'm betting the firing schedule is interesting too.
( I love how one of the comments says it's an ill fitting glaze ... really? )
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#4 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 182
  • Joined: 08-February 12
  • LocationCalifornia

Posted 08 January 2013 - 03:39 PM

i agree, looks like a thick crawl/lichen glaze or similar coating over a colored clay/slip/underglaze. i've never seen one that made such large crawl sections (truly depends on what size the cups actually are) but my guess is this is something that the artist has tested and tweaked a bunch to get the outcome he desires.
0

#5 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 739
  • Joined: 07-December 11
  • LocationCanada

Posted 08 January 2013 - 06:45 PM

View PostChris Campbell, on 08 January 2013 - 01:51 PM, said:

Thanks for sharing this site.
Some look like thick dry lichen glazes which you can find recipes for ... but I have no idea how he does the thick, gluey looking ones.
I'm betting the firing schedule is interesting too.
( I love how one of the comments says it's an ill fitting glaze ... really? )


Yeah Chris, I agree. The glaze doesn't fit very well!
TJR.:Psrc="http://ceramicartsdaily.org/community/public/style_emoticons/default/tongue.gif">
0

#6 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 08 January 2013 - 07:23 PM

He must be applying the glaze very thick to get that type of surface crawl. In addition to the crawling, the satiny surface is especially interesting and nice.
0

#7 User is offline   Brian Reed Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 108
  • Joined: 14-August 12
  • LocationWashington State

Posted 08 January 2013 - 07:34 PM

I have done this by accident on a couple of pots. The crawling white glaze we call "Super Crackle" does this same thing when over a glaze and slightly overfired. The biggest issue was that the super crackle tends to be very sharp and you cannot handle the pots when they over fire like this. I threw them all into the garbage bin.
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club
0

#8 User is offline   claclana Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 55
  • Joined: 17-April 11
  • LocationBuffalo, NY

Posted 08 January 2013 - 10:27 PM

hahah... Brian: it seem so true that ones garbage is a treasure for others! would LOVE to have one of those! not to use, just for the eyes... beauty is food for the soul
thank you all for the ideas!
0

#9 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,399
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 08 January 2013 - 10:53 PM

View PostBrian Reed, on 08 January 2013 - 07:34 PM, said:

I have done this by accident on a couple of pots. The crawling white glaze we call "Super Crackle" does this same thing when over a glaze and slightly overfired. The biggest issue was that the super crackle tends to be very sharp and you cannot handle the pots when they over fire like this. I threw them all into the garbage bin.


Yes, I thought that at first but if you look closely the edges are super smooth ... Also the underglaze colors are on the back of the peeled areas too which suggests a post glaze process or a later cooler firing that only melted the edges? Wierd but wonderful surfaces.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#10 User is offline   SmartsyArtsy Icon

  • Chris Seminara
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 148
  • Joined: 29-October 11
  • LocationPNW

Posted 08 January 2013 - 11:59 PM

One pot has a red glaze applied first but the white crackle over it has blue on its reverse. That's tricky


Chris
Chris Seminara Ceramics
Member, Artisan Tile NorthWest
0

#11 User is offline   Round2potter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 60
  • Joined: 01-December 12
  • LocationPortland, Orygun

Posted 09 January 2013 - 01:05 AM

how would ya'll deal with the problem of glaze chips possibly taking out shelve and stilts?

Super heavy layer of wash?

Scrap bisque tiles under each cup/test series?

i want to do some tests on this! I am thinkin of a carbon trap shino over top a bisque-engobe or my favorite mat glaze
"There is no such thing as cheating in clay; So long as it works"
0

#12 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,399
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 09 January 2013 - 12:19 PM

I would throw a bunch of shallow saucer shapes to catch the glaze run off and buy yourself a grinder to clean the bottoms. Good Luck and post pictures when you get results ... good or bad.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
1

#13 User is offline   weeble Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 100
  • Joined: 12-August 12
  • LocationOregon Coast

Posted 09 January 2013 - 11:20 PM

I'd be interested to actually FEEL that! I wonder if its actually a glaze or maybe something else applied after firing? I have worked with crawling glazes but never that thick, it looks like a lot of fun.
Maryjane Carlson

Whistling Fish Pottery
0

#14 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 739
  • Joined: 07-December 11
  • LocationCanada

Posted 10 January 2013 - 08:45 AM

View PostRound2potter, on 09 January 2013 - 12:05 AM, said:

how would ya'll deal with the problem of glaze chips possibly taking out shelve and stilts?

Super heavy layer of wash?

Scrap bisque tiles under each cup/test series?

i want to do some tests on this! I am thinkin of a carbon trap shino over top a bisque-engobe or my favorite mat glaze


Make yourself some bisque tiles from the same clay body you are using for the bowls. Don't glaze all the way to the foot.
TJR.
0

#15 User is offline   Round2potter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 60
  • Joined: 01-December 12
  • LocationPortland, Orygun

Posted 10 January 2013 - 12:42 PM

Thanks all! i will be sure to post picturtes and my procedure later (also i'll get all my other tests put up too) as soon as the glaze firing schedule allows, For now i think i am gonna stick to simple glazes that i know crawl badly when thick, but i want to lower the flux a little and increase shrinkage (replace flint and flux with spar and i think wollastonite does the trick too, but maybe that works the other way......) i got books books books so it shouldnt be too hard!

Also i really dislike using a mason stain at all (lowfire sculpture ok, but not my wheel work). What is a good strong, stable colorant to start off with for the underglaze, my mind jumps to chrome or cobalt just due to their potency and regularity.

Cheers!

-Burt
"There is no such thing as cheating in clay; So long as it works"
0

#16 User is offline   mregecko Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 47
  • Joined: 14-November 12

Posted 10 January 2013 - 07:56 PM

Are we sure that this is actually achieved with a glaze? I'm of the opinion it's a technique related to the form of the pot, not to heavy glaze crawl, etc.

Look at this image in particular. If this were a glaze crawl, the "back" sides of those peeling pieces would be the same white as the "front"... Instead they are the same red as the under-layer.

Makes me think that this is some elaborately thrown & hand-built work that is glazed very precisely and low fired, to achieve the illusion of heavy crawls.

I could also be very, very wrong. Posted Image
0

#17 User is offline   Diane Puckett Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 203
  • Joined: 18-July 11
  • LocationAsheville, NC

Posted 10 January 2013 - 08:45 PM

View Postmregecko, on 10 January 2013 - 07:56 PM, said:

Are we sure that this is actually achieved with a glaze? I'm of the opinion it's a technique related to the form of the pot, not to heavy glaze crawl, etc.

Look at this image in particular. If this were a glaze crawl, the "back" sides of those peeling pieces would be the same white as the "front"... Instead they are the same red as the under-layer.

Makes me think that this is some elaborately thrown & hand-built work that is glazed very precisely and low fired, to achieve the illusion of heavy crawls.

I could also be very, very wrong. Posted Image

Interesting idea. Like maybe the pot was thrown, then waxed in some places, then covered with a thick porcelain slip that pulled away from the pot and was then manipulated. If the pot was dry before the slip was added, the slip would crack as it started to dry and pull away from the wax. The red color was obviously brushed on.
Diane Puckett
Dry Ridge Pottery
0

#18 User is offline   weeble Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 100
  • Joined: 12-August 12
  • LocationOregon Coast

Posted 12 January 2013 - 05:08 AM

See, I'm still wanting to touch, these COULD be done with something along the lines of a coating of wax or plastic after the firing! A layer of chalky red paint over the pot covered with a wax that shrinks, or ...?

I'm just saying, sort of in a devil's advocate way... I'm reasonably sure they ARE a cool funky glaze, but they don't HAVE to be....
Maryjane Carlson

Whistling Fish Pottery
0

#19 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 12 January 2013 - 05:34 AM

Actually the glaze looks like the 'Lamb's Fat' glaze or what TJ called 'Mutton Fat' glaze. The 'creamier' of the textures looks exactly like it.

The last time I saw the glaze it was in an issue of CM (years and years and years ago). The glaze flowed thickly and dripped over the rim. The translucency was almost like magnesia but thicker and white with a tinge of blue; fantastic.
INRI
0

#20 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,500
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 12 January 2013 - 12:00 PM

For crawling and bead glazes, increase additions of magnesium carbonate. Try incremental increases 2-3% and the crawling can eventually develop in raised beads.
Marcia
Marcia Selsor
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users