Hello,

after my first pitfiring last year I'm not sure if there's a difference... I thought himalaja salt is better (more minerals) but it is more expensive.

What do you say, is there a difference between table salt and himalaja salt when using in pit or barrel firing? Any viewable results? As I'm said, I'm not sure, as from a chemical point of view they are the same...

Kind regards

J.P.
0

#2 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 138
  • Joined: 20-May 12
  • LocationColorado

Posted 07 January 2013 - 09:54 PM

I really don't think there should be a difference, as long as you are adding sodium and potassium to the pit both naturally and chemicly the sodium will give you the same result, sodium is too reliable to be that touchey.
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#3 User is offline   Iforgot Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 138
  • Joined: 20-May 12
  • LocationColorado

Posted 07 January 2013 - 09:59 PM

And visually, no matter if it's sodium, potassium, or copper the forms really do effect the final piece, but himmalya salt is kind of a waste of money.
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#4 User is offline   Evertier Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 07-January 13

Posted 10 January 2013 - 07:03 PM

Thank you very much for your answer - and I'm very sorry for responding so late.
So I'll use next time only the cheaper table salt instead of the himalaya one.