Can anyone give me a cost effective brand name and source for spray guns/ spray booth to use in glaze application? Are the bottom cannister spray guns better/easier to handle when spraying for an extensive length of time?
0

#2 User is offline   Seasoned Warrior Icon

  • Businessman - Potter
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 294
  • Joined: 02-April 10

Posted 26 July 2010 - 04:40 PM

View PostMMFOWV, on 26 July 2010 - 11:27 AM, said:

Can anyone give me a cost effective brand name and source for spray guns/ spray booth to use in glaze application? Are the bottom cannister spray guns better/easier to handle when spraying for an extensive length of time?


my personal favorite is he Paasche 62, check it out at http://www.chicagoai...m/pa62sphe.html

I've also seen a lot of ggod thinggs about a detail sprayer with a gravity feed available Habor Freight. I've never used it but a lot seem to like it. I think the orifice would be too small and glog frequently but a lot do like it.

The Paasche uses less air and you can use a variety of bottles on the siphone. I like the squeeze type ketchup bottles one finds in a restaurant (or restaurant supply house) which are cheap and are larger than the the one that comes with the sprayer. You also need to replace the small pick-up tube because with the larger bottles it too short. great sprayer, easy clean up and failproof.

Regards
Charles
0

#3 User is offline   ArtView Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 83
  • Joined: 03-May 10
  • LocationMooresville & Boone, NC

Posted 27 July 2010 - 09:56 PM

Great spray gun from Bailey. Advantage is the mechanical parts do not wear out from glaze chemicals...also, does not clog as often. Tip: buy extra containers for quick glaze changeovers.

Bailey Spray Gun

Based on research, this is my favorite spray booth....depends on your needs:

Spray Booth

and if you are pretty handy...a homemade idea....(my understanding is that you can get really creative with a squirrel cage - I think that is the name--from an HVAC parts supplies/company)

Homemade spray booth

Good luck!!
Lee Ann Harrison
Student Board Member - Potters Council

Artview Studio, Inc.
http://www.artviewstudio.com/
http://twitter.com/artviewstudio
http://www.facebook.com/artview.studio
and one last website:
http://www.artstoryboarding.com
0

#4 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,435
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 29 July 2010 - 01:54 PM

I use an "E-Z" sprayer that I got from Archie Bray Clay business ages ago. I have 4 additional jars for quickly changing glazes while spraying. It is a simple syphon sprayer/ I also use a Paasche air brush for applying underglazes. I have an old power pal compressor from Sears that I have also had for ages.
Marcia Selsor