Interesting -- don't give up "grandma's" pyrex. Lessons on changes in basic materials and following directions regarding use apply to clay, also.

http://todayhealth.t...n-the-rise?lite
0

#2 User is offline   Diana Ferreira Icon

  • opinionated ignoramus
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 180
  • Joined: 21-October 11
  • LocationCape Town, South Africa

Posted 21 December 2012 - 10:37 AM

yea, old Pyrex used to be made of Borosilicate glass. Sadly not today.
Diana
www.dianaferreiraceramics.com
https://www.facebook...70824173&type=3
0

#3 User is online   Diane Puckett Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 174
  • Joined: 18-July 11
  • LocationAsheville, NC

Posted 21 December 2012 - 04:37 PM

Interesting article. Now I know it is not me just imagining the difference in newer Pyrex. In addition, the numbers came off my new Pyrex measuring cup I when I ran it through the dishwasher, and another Pyrex measuring cup dribbles when it pours. That was aggravating, but now I am afraid to even use them in the microwave.
Diane Puckett
Dry Ridge Pottery
0

#4 User is offline   Mark McCombs Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 110
  • Joined: 13-August 12
  • LocationSW Washington

Posted 21 December 2012 - 10:14 PM

I found this out the hard way several years ago.
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users