Hi, need some expert advice please! So I am ready to get the kiln set up and I have two questions.

I am having a cover built for it over a concrete pad - roof, no walls, and need to know how high it needs to be. This is the kiln, most likely it's Crucible:

Posted Image
Also how big of a gas tank should I get for it? Will 150 gallons be enough? Or should I get 250?

Thanks, this is my first kiln and I just want to make sure it is set up right!
0

#2 User is offline   porcelainsculptor Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 22
  • Joined: 08-September 11

Posted 13 December 2012 - 03:52 PM

Well I went with a 150 gallon tank and eight foot roof! Hope that does the trick....
0

#3 User is offline   Rakuken Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 25
  • Joined: 09-December 11
  • LocationHawaii

Posted 13 December 2012 - 07:39 PM

View Postporcelainsculptor, on 13 December 2012 - 10:52 AM, said:

Well I went with a 150 gallon tank and eight foot roof! Hope that does the trick....


My roof is corrugated metal. The height is 20 inches above the kiln with a fiber shield. When I fired with only one collar extension the distance from the top of the kiln to the roof was 30 inches without the fiber shield, I fired it that way for 8 years.

Attached File(s)


0

#4 User is offline   porcelainsculptor Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 22
  • Joined: 08-September 11

Posted 13 December 2012 - 07:51 PM

View PostRakuken, on 13 December 2012 - 07:39 PM, said:

View Postporcelainsculptor, on 13 December 2012 - 10:52 AM, said:

Well I went with a 150 gallon tank and eight foot roof! Hope that does the trick....


My roof is corrugated metal. The height is 20 inches above the kiln with a fiber shield. When I fired with only one collar extension the distance from the top of the kiln to the roof was 30 inches without the fiber shield, I fired it that way for 8 years.


Thanks for the response. Do you think I need to get a fiber shield?
0

#5 User is offline   Brian Reed Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 108
  • Joined: 14-August 12
  • LocationWashington State

Posted 13 December 2012 - 11:17 PM

I have the same kiln, although I have a small extender ring that makes it slighly larger. I fire it with two 100lb (25 gal) tanks plumbed in tandem and it works great. I build a hood out of galvanized steel to vent the heat instead. Make sure you put in a baffle shelf when you load it and know that the top shelf is going to be much cooler than the rest of the kiln. I fire ^10 reduction everytime now that I have it dialed in. Put two shelf pieces to block the vent hole as a damper with only about 2 inches open when you want to start reduction.



Good luck.
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club
0

#6 User is offline   porcelainsculptor Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 22
  • Joined: 08-September 11

Posted 14 December 2012 - 12:03 AM

View PostBrian Reed, on 13 December 2012 - 11:17 PM, said:

I have the same kiln, although I have a small extender ring that makes it slighly larger. I fire it with two 100lb (25 gal) tanks plumbed in tandem and it works great. I build a hood out of galvanized steel to vent the heat instead. Make sure you put in a baffle shelf when you load it and know that the top shelf is going to be much cooler than the rest of the kiln. I fire ^10 reduction everytime now that I have it dialed in. Put two shelf pieces to block the vent hole as a damper with only about 2 inches open when you want to start reduction.



Good luck.


Thanks for the info Brian. I am beginning to realize how little I know about this and it is making me a bit nervous - can you recommend a book maybe?
0

#7 User is offline   Brian Reed Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 108
  • Joined: 14-August 12
  • LocationWashington State

Posted 14 December 2012 - 11:33 AM

Unfortunately I do not know of any books, nor have any books on how to learn to fire a gas kiln. I had some advice from people I know and the two page instructions from Seattle Pottery Supply. the rest was trial and error over a course of firing.



Good luck and keep practicing.
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club
0

#8 User is offline   justanassembler Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 144
  • Joined: 16-May 11
  • LocationBaton Rouge, LA

Posted 14 December 2012 - 12:54 PM

Nils Lou's book, The Art of Firing has some good information in it, if I recall correctly.