I had made a big tile and it's plaster mold, I didn't take it off and the clay is almost dry
and do not know how to remove it, I wish not to hurt the plaster in the process, do you some suggestions?
THANKS!
Page 1 of 1
remove clay from plaster mold almost dry clay
#3
Posted 12 December 2012 - 04:15 PM
yeah, you can soften the clay up a bit and try to remove - but you'll have to dry it out longer to cure the mold before using. i recommend trying to use an air hose if you have access to air compressor - stream your air between the clay and plaster to try to release w/o damaging the plaster with tools. you can also use a damp sponge to remove clay from your plaster.