: What is the best way to cut a chimney -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

What is the best way to cut a chimney Rate Topic: -----

#1 User is offline   Idahopotter Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 11
  • Joined: 10-December 12

Posted 11 December 2012 - 01:42 PM

So I have an electric kiln that i am converting to gas and I need to cut a chimney in the top. The top is a harder metal not your typical electric kiln soft metal. How should I go about cutting it
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 11 December 2012 - 02:21 PM

Here are some ideas-grind it with a diamond 4 inch cut off blade
Drill starter hole on a corner and sawzall with metal blade.This may shake more than you want.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is online   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,503
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 11 December 2012 - 03:12 PM

I'd remove the lid and set the outer parts on dry clay bags or sand bags or something to absorb the vibration.
Marcia
Marcia Selsor
0

#4 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 182
  • Joined: 08-February 12
  • LocationCalifornia

Posted 11 December 2012 - 04:15 PM

harder "metal" (like the metal jacket on a kiln) or did you mean harder soft brick? if so, this is because it's got a refractory mortar/coating on it, and it's just a coating. beyond this is soft brick which is easily cut with pretty much any saw.

if it's metal - i would use a standard cutoff wheel (not diamond) on the metal to get through the jacket, then switch to a sawzall or hand saw (or even hole saw) for getting through the soft brick.

removing the lid and putting it on surface that will absorb vibrations will be smart as well. good luck!
0

#5 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 11 December 2012 - 04:39 PM

View PostIdahopotter, on 11 December 2012 - 01:42 PM, said:

So I have an electric kiln that i am converting to gas and I need to cut a chimney in the top. The top is a harder metal not your typical electric kiln soft metal. How should I go about cutting it

Since you only asked about metal
I'm assuming it stainless steel-but thats not over the lid top usually unless its an old square cress or other brand. The soft brick will cut like butter
I do agree on Perkos standard cutoff wheel suggestion.That should cut just about anything.
Wear eye and ear protection
Mark
Mark Cortright
www.liscomhillpottery.com
0

#6 User is offline   Idahopotter Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 11
  • Joined: 10-December 12

Posted 11 December 2012 - 04:52 PM

View PostMark C., on 11 December 2012 - 02:39 PM, said:

View PostIdahopotter, on 11 December 2012 - 01:42 PM, said:

So I have an electric kiln that i am converting to gas and I need to cut a chimney in the top. The top is a harder metal not your typical electric kiln soft metal. How should I go about cutting it

Since you only asked about metal
I'm assuming it stainless steel-but thats not over the lid top usually unless its an old square cress or other brand. The soft brick will cut like butter
I do agree on Perkos standard cutoff wheel suggestion.That should cut just about anything.
Wear eye and ear protection
Mark


This is one of those old square cress kilns
0

#7 User is online   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,503
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 11 December 2012 - 05:36 PM

so can you separate the metal from the brick on the lid in order to cut a flue /chimney hole or no? It is kind of difficult to advise without the full picture.


Marcia
Marcia Selsor
0

#8 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 182
  • Joined: 08-February 12
  • LocationCalifornia

Posted 11 December 2012 - 07:07 PM

yeah, cutoff wheel on a grinder will cut through that thin sheet metal like butter. if you don't want the hole in the brick exactly where your hole in the jacket is at, you can try to score the metal with the grinder (if you have the dexterity) until you just barely make it through, then cut your brick hole wherever you want. either way, should be easy.

i doubt the metal will be easily separated from the kiln - age and fatigue from heat cycles will make it difficult and most likely brittle. i'd leave it in place for this task.
0

#9 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 11 December 2012 - 07:23 PM

Cut thru the metal larger hole than you need so metal is not near exhaust hole. Then with hole saw (hand saw) cut the bricks. Those old cress kiln are build like tanks-weigh a ton and last forever.
Mark
Mark Cortright