Bisque Misfire? I set the knobs incorrectly.. Rate Topic: -----

#1 User is offline   paige Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 11-December 12

Posted 11 December 2012 - 09:53 AM

Yesterday I fired my Paragon snf243 - attempting cone 05, no watcher - and I set the knobs incorrectly. They should have been 5 - 1- 2, for 5 -6 hours, but I did 1 - 1- 2 for 7 hours. I don't know why my brain wasn't working, but that's another problem entirely. The kiln sitter never tripped and the little cone doesn't appear to have bent.

Should I refire or assume that it still got pretty hot enough? What does that first (top) knob determine?

Thanks for the help!
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,445
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 11 December 2012 - 09:57 AM

I am not familiar with what 5-1-2 or 1-1-5 is.
But if you didn't hit temperature, just refire using the right settings. If it doesn't work a second time, maybe you need new elements.

Marcia
Marcia Selsor
0

#3 User is offline   paige Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 11-December 12

Posted 11 December 2012 - 10:20 AM

Well that first knob is the power level, so at min setting, I doubt it got very hot. I just restarted it. Oi.

View PostMarcia Selsor, on 11 December 2012 - 09:57 AM, said:

I am not familiar with what 5-1-2 or 1-1-5 is.
But if you didn't hit temperature, just refire using the right settings. If it doesn't work a second time, maybe you need new elements.

Marcia

0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users