an experiment not to repeat Cuisinart noodle maker as a small-scale power extruder Rate Topic: -----

#1 User is offline   docweathers Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 180
  • Joined: 30-July 11
  • LocationSpokane Wa

Posted 10 December 2012 - 09:19 PM

If you've ever been tempted to try your wife's Cuisinart noodle maker as a small-scale power extruder, don't do it. I gave it a try today and the most important outcome was cleaning up a huge mess. The dies are much too small, require very soft clay, and are almost impossible to clean out. I will stick with my Northstar from now on:unsure:src="http://ceramicartsdaily.org/community/public/style_emoticons/default/unsure.gif">
Lawrence Weathers
Spokane Wa
Returning to pottery after 40 years absence
Welded Sculpture
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,346
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 10 December 2012 - 09:30 PM

I always think of Cuisinart right up with Brent Shimpo Northstar Bailey Soldner.
Now on a more realist note the best power kitchen item I can suggest is your blender (thrift/yard sale best)
this makes short work of small test glazes and non easy screenable materials like zinc or bentonite.
This is where a Cuisinart blender will shine-just make sure it never goes back into the kitchen again after use.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is online   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 917
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 11 December 2012 - 09:07 AM

View PostMark C., on 10 December 2012 - 09:30 PM, said:

I always think of Cuisinart right up with Brent Shimpo Northstar Bailey Soldner.
Now on a more realist note the best power kitchen item I can suggest is your blender (thrift/yard sale best)
this makes short work of small test glazes and non easy screenable materials like zinc or bentonite.
This is where a Cuisinart blender will shine-just make sure it never goes back into the kitchen again after use.
Mark


I bought a cheap blender to use making paperclay and burned it out quickly. Now, I sneak into the kitchen to get the Cuisinart. I've used it for over a year and still have not burned it out. I clean it up after each use and put it back in the kitchen without my wife knowing.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#4 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 695
  • Joined: 07-December 11
  • LocationCanada

Posted 11 December 2012 - 10:14 AM

View PostOffCenter, on 11 December 2012 - 08:07 AM, said:

View PostMark C., on 10 December 2012 - 09:30 PM, said:

I always think of Cuisinart right up with Brent Shimpo Northstar Bailey Soldner.
Now on a more realist note the best power kitchen item I can suggest is your blender (thrift/yard sale best)
this makes short work of small test glazes and non easy screenable materials like zinc or bentonite.
This is where a Cuisinart blender will shine-just make sure it never goes back into the kitchen again after use.
Mark


I bought a cheap blender to use making paperclay and burned it out quickly. Now, I sneak into the kitchen to get the Cuisinart. I've used it for over a year and still have not burned it out. I clean it up after each use and put it back in the kitchen without my wife knowing.

Jim

Jim;
A blender is not good for making paper, or paper clay. I burned out about 5 of them in one year. Then it hit me! I am a potter! I have the technology! Now I use a 5 gallon pail, slake my materials overnight, then use my big plaster mixer on my variable speed drill. Works fabulously. Is that a word?
TJR.
0

#5 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 695
  • Joined: 07-December 11
  • LocationCanada

Posted 11 December 2012 - 10:19 AM

View Postdocweathers, on 10 December 2012 - 08:19 PM, said:

If you've ever been tempted to try your wife's Cuisinart noodle maker as a small-scale power extruder, don't do it. I gave it a try today and the most important outcome was cleaning up a huge mess. The dies are much too small, require very soft clay, and are almost impossible to clean out. I will stick with my Northstar from now on:unsure:src="http://ceramicartsdaily.org/community/public/style_emoticons/default/unsure.gif">


DOCWEATHERS;
MY DAD USED TO COME INTO THE KITCHEN AND GRAB A WOODEN SPOON IF HE NEEDED A PIECE OF DOWEL. I ALWAYS WONDERED WHY, AS I GREW UP, all the spoons had short handles. If you like being married to your current wife, I would stay out of the kitchen, and haunt garage sales.My parents remained married, but this always came up in conversation.I buy my own wooden spoons.
TJR.
0

#6 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 171
  • Joined: 08-February 12
  • LocationCalifornia

Posted 11 December 2012 - 04:28 PM

View PostTJR, on 11 December 2012 - 07:14 AM, said:

A blender is not good for making paper, or paper clay. I burned out about 5 of them in one year.


a Vita Mix blender will handle chopping up paper all day long. had a Grad student last year who was grinding up her old mail into pulp to make paper and paper mache for her sculptures for like 3 months. she literally blended hundreds of pounds of paper through this thing. it was an OLD Vita Mix from a garage sale - when she finally though she killed it she gave me the vita mix to diagnose and see if it could be repaired while she was out buying a cheap replacement blender....found out it just blew the fuse inside the housing....good to go for the rest of her project Posted Image i've literally watched these blenders chop up a broomstick, 2x2 wood blocks, cell phone, and many other things during a demo and online videos.