What happens to wax resist in a kiln? Rate Topic: -----

#1 User is offline   justin1287 Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 41
  • Joined: 15-October 12

Posted 28 November 2012 - 01:40 PM

does it completely evaporate, or does it leave residue left behind?
0

#2 User is online   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,442
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 28 November 2012 - 02:26 PM

Yes, it should completely burn off.

Marcia
Marcia Selsor
0

#3 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 698
  • Joined: 07-December 11
  • LocationCanada

Posted 28 November 2012 - 07:10 PM

Should burn off. Make sure your kiln is vented.
Tom.[TJR]
0