: Curvy hollow tubes -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Curvy hollow tubes Rate Topic: -----

#1 User is offline   justin1287 Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 41
  • Joined: 15-October 12

Posted 28 November 2012 - 01:14 PM

so, is there something i can wrap clay around that will disinigrate when firing that is soft and moldable? i want to make hollow curvy tubes......but if i put something in the middle that is hard, the clay will crack cause it will shrink.

thx

justin
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,494
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 28 November 2012 - 02:22 PM

If you take a tube, wrap paper around it. Wrap the clay around it. Slide the tube out of the paper and clay wrap.
Done! I do this for large tubes 8" x 28" ht with a tarpaper outside wrap. For smaller pieces the tar paper isn't necessary. I do remover the tar paper after it sits overnight. You can still manipulate it while it is soft leather hard.

Attached File(s)


Marcia Selsor
0

#3 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,398
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 28 November 2012 - 04:13 PM

Another idea I've used is to fill a nylon stocking or children's balloon with sand to get it to a tube shape then fashion the clay around it.
When it sets up a bit just open the end and dump out the sand. This works very well for any soft flowing forms ... also for fat vases with tiny openings.
Sometimes you can just fill up the balloon with air, but if you are going to roll it and work on a form, use sand to avoid the chance of bursting the balloon.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#4 User is offline   Cass Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 155
  • Joined: 12-September 12
  • LocationMontana

Posted 28 November 2012 - 06:01 PM

how about the balloons a clown would make animals from, then pop it
0

#5 User is offline   justin1287 Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 41
  • Joined: 15-October 12

Posted 29 November 2012 - 01:46 AM

Thx....I,ve done the paper thing.....i like the balloon idea as well. Thanks for sharing!
0

#6 User is offline   minspargal Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 60
  • Joined: 21-February 11
  • LocationPort Aransas, Tx

Posted 29 November 2012 - 08:42 AM

i like the stocking idea, never thought of that for free flowing hollow shapes.
0

#7 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,398
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 29 November 2012 - 11:18 AM

One downside to the nylons is that sand dust can pass through and leave marks ... they are not terrible, just something to know if you want the inner surface to be smooth.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#8 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,494
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 29 November 2012 - 11:40 AM

James Melchert used vermiculite in stocking for curvy tubes. Vrmiculite is considered hazardous now because of possible asbestos content.
Maybe something that would not leak through the stocking would be perlite granules. It is lighter weight than sand.

Marcia
Marcia Selsor
0

#9 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 29 November 2012 - 02:36 PM

You can use an extruder . . . curl and shape the tubes as they come out. Different size dies will give you different size tubes.
0

#10 User is offline   weeble Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 100
  • Joined: 12-August 12
  • LocationOregon Coast

Posted 02 December 2012 - 03:06 AM

OH! I like the idea of the nylon full of sand for a project I've been wanting to do! I tried a balloon, but had a heck of a time getting anything inside, and without something inside it is just too squishy and deforms, so my project self destructed.

Now I need to locate some old knee-highs or something... MMMmmmmmmm
Maryjane Carlson

Whistling Fish Pottery
0

#11 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,494
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 02 December 2012 - 08:36 AM

View Postbciskepottery, on 29 November 2012 - 01:36 PM, said:

You can use an extruder . . . curl and shape the tubes as they come out. Different size dies will give you different size tubes.


you're right. I was thinking bigger than the capacity of my extruder. Your answer is so simple and evident I missed even thinking of it.
Good idea.!
Marcia
Marcia Selsor
0

#12 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,494
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 02 December 2012 - 08:37 AM

when I changed cat boxes yesterday, I thought of this thread and thought kitty litter is lighter weight than sand and easily available. Also large enough not to leak out of pantyhose.
Marcia


Marcia Selsor
0

#13 User is offline   minspargal Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 60
  • Joined: 21-February 11
  • LocationPort Aransas, Tx

Posted 02 December 2012 - 08:48 AM

View PostMarcia Selsor, on 02 December 2012 - 07:37 AM, said:

when I changed cat boxes yesterday, I thought of this thread and thought kitty litter is lighter weight than sand and easily available. Also large enough not to leak out of pantyhose.
Marcia


Cat litter, good idea...easier to find than the other two things mentioned. We have sand every where here but it is soooo fine it would go thru the stockings. And i finally have a use for all those ruined panty hose, now i can make my mermaid!
0

#14 User is offline   Pres Icon

  • Advanced Member
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,095
  • Joined: 02-April 10
  • LocationCentral, PA

Posted 03 December 2012 - 09:31 AM

View PostChris Campbell, on 29 November 2012 - 11:18 AM, said:

One downside to the nylons is that sand dust can pass through and leave marks ... they are not terrible, just something to know if you want the inner surface to be smooth.


The sand dust does go through the stockings, this can be cut back if you use the stockings made for diabetics or people with leg circulation problems. The denser weave will cut back on the dust.