I just tried glass bead media for attempting to get a "mat" finish on a piece. It etched in further than I would like. Has anyone used walnut shell media?
0

#2 User is online   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 25 November 2012 - 03:46 PM

Depends on the glaze? How hard it is? (what its made of-like some colbalt glazes and reds are very soft)
what its fired to cone wise?
This may not be what you want to do but how about putting a Matt glaze on to begin with?
Walnut shells work great on painted wood and metal and are less aggressive than glass beads.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   buckbuck Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 13
  • Joined: 24-December 10
  • LocationAirway Heights, WA

Posted 25 November 2012 - 03:48 PM

The glaze I'm working on is a crackle. I want to make a contrast between gloss and mat.
0

#4 User is offline   buckbuck Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 13
  • Joined: 24-December 10
  • LocationAirway Heights, WA

Posted 25 November 2012 - 03:49 PM

It is a cone 6 and inked.
0

#5 User is online   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 25 November 2012 - 04:04 PM

I would try the shells and if its to aggressive enough add a very small amount of silica sand to them (small mesh size)
Mark
Mark Cortright
www.liscomhillpottery.com
0

#6 User is offline   buckbuck Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 13
  • Joined: 24-December 10
  • LocationAirway Heights, WA

Posted 25 November 2012 - 04:17 PM

Thank you. I will give it a try. I had to pick someting and got the glass bead. Next trip will be Walnut. Any suggestions if I have a choice on size? After I try it I'll post the results.
0

#7 User is offline   scoobydoozie Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 130
  • Joined: 16-August 11
  • LocationClearwater, FL

Posted 26 November 2012 - 08:28 AM

Try glass etching cream. Much easier...
0

#8 User is offline   minspargal Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 60
  • Joined: 21-February 11
  • LocationPort Aransas, Tx

Posted 26 November 2012 - 09:04 AM

Never heard of etching cream, where does one find it?
0

#9 User is offline   Denice Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 470
  • Joined: 02-April 10
  • LocationWichita, Kansas

Posted 26 November 2012 - 09:09 AM

You can find glass etching cream at craft stores all we have here is hobby lobby and Michaels. It's easier, cleaner and you can matt small areas with it. Denice
0