Posted 17 November 2012 - 11:27 AM

I'm new at this. I fired a piece recently and used two different glazes - one says to fire at cone 5/6. The other says to fire at cone 05/06.
the low temperature glaze did OK. The higher temperature glaze seems to have completely disappeared. I would say it was overfired, but the 05/06 glaze did fine. What happened?

If glazes need to fire at different temperatures do you just fire them at different times or can they never be used together on the same piece?
0

#2 User is offline   Mark McCombs Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 110
  • Joined: 13-August 12
  • LocationSW Washington

Posted 17 November 2012 - 12:37 PM

What cone did you fire the pieces to?

And yes, you would fire them separately as there is a great difference in temperature between cone 05 and cone 6.

You either overfired one of the glazes or underfired the other.
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt
0

#3 User is offline   Diane Puckett Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 173
  • Joined: 18-July 11
  • LocationAsheville, NC

Posted 17 November 2012 - 04:06 PM

There are excellent books on glazing and firing. My favorites are John Britt's Complete Guide to High Fire Glazes, Mark Burleson's The Ceramic Glaze Handbook, Robin Hopper's The Ceramic Spectrum, and Hesselberth & Roy's Mastering Cone Six Glazes.

Also check out http://digitalfire.c..._cones_193.html
Diane Puckett
Dry Ridge Pottery
0

#4 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 18 November 2012 - 02:34 AM

View Postsoyarsm, on 17 November 2012 - 08:27 AM, said:

I'm new at this. I fired a piece recently and used two different glazes - one says to fire at cone 5/6. The other says to fire at cone 05/06.
the low temperature glaze did OK. The higher temperature glaze seems to have completely disappeared. I would say it was overfired, but the 05/06 glaze did fine. What happened?

If glazes need to fire at different temperatures do you just fire them at different times or can they never be used together on the same piece?



The Cone 05-06 did fine you say and the Cone 5/6 disappeared? It sounds as if you fired low and the high fire glaze is underfired and has changed color only. When firing multiple temperature glazes on one piece, fire the highest temperature glaze first, then apply and fire your lower firing glaze(s). If it were reversed, if you fired high first, the high firing glaze would have been fine and the lower temperature glaze would most likely have bubbles, or may be excessively runny or have some other glaze defect from being overfired.


INRI
0

#5 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,431
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 18 November 2012 - 10:22 PM

If you wanted to use both glazes on the same piece, you would need to fire the higher temperature glaze (5-6) first. Then apply the lower temperature glaze(05-06) and fire the low temperature.
Marcia
Marcia Selsor
0

#6 User is offline   Ben Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 113
  • Joined: 10-November 10

Posted 23 November 2012 - 10:15 AM

Cones measure heat work. That is not exactly temperature but we simplify it to say that at a given rate of temp climb (say 250f/hour) a given cone will equal a given temperature.
Cones were originally numbered in such a way that they didn't go down to room temperature so they had to go below cone zero. SO, they added a zero to the front of the number and began counting backwards. Therefore, cone 05 is about an equal distance below cone 0 as cone 5 is above.
Do a web search for a cone chart. I have one saved on my computer and several printed out around the studio. You'll be able to see how much difference there is in 05 and 5.

Ben
0

#7 User is offline   soyarsm Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 17-November 12

Posted 24 November 2012 - 08:51 AM

View PostLucille Oka, on 18 November 2012 - 02:34 AM, said:

View Postsoyarsm, on 17 November 2012 - 08:27 AM, said:

I'm new at this. I fired a piece recently and used two different glazes - one says to fire at cone 5/6. The other says to fire at cone 05/06.
the low temperature glaze did OK. The higher temperature glaze seems to have completely disappeared. I would say it was overfired, but the 05/06 glaze did fine. What happened?

If glazes need to fire at different temperatures do you just fire them at different times or can they never be used together on the same piece?



The Cone 05-06 did fine you say and the Cone 5/6 disappeared? It sounds as if you fired low and the high fire glaze is underfired and has changed color only. When firing multiple temperature glazes on one piece, fire the highest temperature glaze first, then apply and fire your lower firing glaze(s). If it were reversed, if you fired high first, the high firing glaze would have been fine and the lower temperature glaze would most likely have bubbles, or may be excessively runny or have some other glaze defect from being overfired.