: Can you stack kilns? -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Can you stack kilns? Rate Topic: -----

#1 User is offline   Nightshade Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 20
  • Joined: 16-March 12
  • LocationOhio

Posted 16 November 2012 - 07:04 PM

Ok, so I found two kilns that fire the same. They are the smaller ones that come in sections. This might be a dumb question but could I stack them to have a taller kiln? Just a thought. Any feedback is appreciated.
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,366
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 16 November 2012 - 10:56 PM

View PostNightshade, on 16 November 2012 - 07:04 PM, said:

Ok, so I found two kilns that fire the same. They are the smaller ones that come in sections. This might be a dumb question but could I stack them to have a taller kiln? Just a thought. Any feedback is appreciated.


Are these electrics? gas? same brand ?how many amps?-same plugs? dead rings?Need more info?
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   Cass Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 155
  • Joined: 12-September 12
  • LocationMontana

Posted 16 November 2012 - 11:23 PM

sounds doable if they are the same model/specs...i would find an adventurous independent kiln tech or electrician ( if we are talking about electric)
0

#4 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 17 November 2012 - 05:11 AM

I do not know the ins and outs of such a configuration but Skutt does. You can ask them about the Transformer package and see if it is available to you and if it will work for you. Don't forget to watch the video- http://www.skutt.com/transformer/
INRI
0

#5 User is offline   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 984
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 17 November 2012 - 10:23 AM

During my first incarnation as a potter in Denver during the '70 I sometimes helped a sculptor fire her pieces by adding one or two sections of one kiln to another kiln. They were the same model (probably either Skutt or Paragon).

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#6 User is offline   perkolator Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 179
  • Joined: 08-February 12
  • LocationCalifornia

Posted 19 November 2012 - 06:04 PM

yes it CAN be done if you have a means to safely power those additional sections - i'm sure you may already know, you can't just simply plug them into the same control box (unless it was designed for this).