I would like to mix a porcelain clay body with a stoneware clay body.
Has anybody tried this before?
What happens after a bisque fire?
Which temperature do you follow for the bisque & glaze fire - the porcelain body or the stoneware?
When it comes to glazing, can I use an earthenware premixed glaze on this mixed body?
Will it be food safe if I leave it unglazed?

Thanks for any advice most welcome! I haven't a clue.


0

#2 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 16 November 2012 - 06:53 AM

Many clay manufacturers sell a blend of porcelain/stoneware, often a 50/50 mix. Look for compatibility in shrinkage; do some small test batches and bisque and glaze fire to see how they perform before going an committing yourself to large amounts. I would mix cone 6 porcelain with cone 6 stoneware, cone 10 porcelain with cone 10 stoneware.

Foods safe for unglazed will depend on firing to maturity and surface and what is in the clay bodies . . . something that is rough and pitted, or carved, will offer hiding places for bacteria to grow and fester. You can always put a napkin or other item between food and surface. Restrict yourself to non-liquids, etc. Foods may stain the surface.
0

#3 User is online   clay lover Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 405
  • Joined: 08-April 10

Posted 16 November 2012 - 08:49 AM

I often mix a % of porcelain, ^6, in with my ^6 stoneware clay to get better throwability, or lighten the color, or reduce the speckles of the stoneware. Sometimes I leave it only semi-mixed, and have swirles in the light-dark clay that make a good look on the finished piece.
0

#4 User is offline   Essaily Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 20
  • Joined: 25-May 12

Posted 17 November 2012 - 05:46 AM

Thanks all for your informative posts! I looked at the packaging and noticed it is already mixed with stoneware. Let's see what happens.