vitrified unglazed pottery and food Is it safe to be use for food?

#1 User is offline   cambriapottery Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 22
  • Joined: 19-April 11
  • LocationCanada

Posted 15 November 2012 - 10:41 PM

In general is it unsafe to use unglazed stoneware for food?
0

#2 User is offline   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 958
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 15 November 2012 - 10:47 PM

View Postcambriapottery, on 15 November 2012 - 10:41 PM, said:

In general is it unsafe to use unglazed stoneware for food?


No.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#3 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,491
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 16 November 2012 - 10:32 AM

What he said.

best,

....................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#4 User is offline   bciskepottery Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 753
  • Joined: 28-June 10

Posted 16 November 2012 - 11:02 AM

Little confused by the syntax . . . unsafe to use unglazed or safe to use unglazed? What kind of food -- dry (breads, etc) or liquid (soups, sauces, etc)?

There have been a few posts lately about using unglazed for food . . . the thought of a knife or spoon scraping across an unglazed surface is giving me flashbacks school days and fingernails skreeching across the blackboard.
0

#5 User is offline   Nancy S. Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 62
  • Joined: 05-September 12

Posted 16 November 2012 - 02:56 PM

View Postbciskepottery, on 16 November 2012 - 11:02 AM, said:

Little confused by the syntax . . . unsafe to use unglazed or safe to use unglazed? What kind of food -- dry (breads, etc) or liquid (soups, sauces, etc)?

There have been a few posts lately about using unglazed for food . . . the thought of a knife or spoon scraping across an unglazed surface is giving me flashbacks school days and fingernails skreeching across the blackboard.


*laughs* Oh, man! You just made my skin crawl... O_o

I use unglazed ^6 clay, fired to ^6, for salt piggies. Seems to work pretty well. I also use the same clay only fired to ^06 (more absorbent that way) for sugar keepers - also works well. So while they're not in contact with liquids, they're also not being used with utensils.
0

#6 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,491
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 16 November 2012 - 03:12 PM

Not everyone uses metal eating implements, nor does everyone use forks, spoons, and knives.

best,

...................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#7 User is offline   koreyej Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 47
  • Joined: 03-May 12
  • LocationBouton, Iowa

Posted 20 November 2012 - 12:16 PM

Funny question. Isn't that what Pampered Chef's ware is? Personally, I like my ware glazed. However, they offer a lot of ovenware that is not glazed and sell it as food safe. Maybe worthy of some investigation?
Korey Averill
ka Studios Pottery

www.facebook.com/kastudiospottery
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users