orange peel for cone 9 glaze formula

#1 User is offline   Diane Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 4
  • Joined: 29-July 11
  • LocationNY

Posted 11 November 2012 - 04:17 PM

Hi everyone,
Looking for an orange peel glaze for cone 9...is there any such thing? Working in porcelain...
0

#2 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,491
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 12 November 2012 - 10:03 AM

A salt kiln? ;)

best,

..............john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users