Hello,
I just bought a Duncan 1029-2. The bricks seem to be in good shape other than the lid and the floor. They seem to be made of some other material than the usual brick used in kilns and I have never seen anything like it. It seems to be disintegrating and looks similar to a fiber blanket material. Does anyone know what it is? Does anyone know if replacing the lid and the floor with regular kiln brick will work?
Thank you for your help!
Heather
Page 1 of 1
Duncan Kiln 1029 -strange material lid and floor
#2
Posted 11 November 2012 - 12:54 AM
A photo would really help in this.
Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??
Mark
Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??
Mark
Mark Cortright
www.liscomhillpottery.com
www.liscomhillpottery.com
#3
Posted 11 November 2012 - 05:14 PM
Get some insulating fire brick, (soft bricks), and replace the floor and lid, that should work fine.
STEPHEN ROBISON
Head of Ceramics, Central Washington University
Ellensburg WA
http://stiffyguss.blogspot.com/
http://liquidceramics.blogspot.com/
http://teapotspitchers.blogspot.com/
http://woodkilns.blogspot.com/
http://jomonhaniwa.blogspot.com/
http://stephensrobison.blogspot.com/
http://www.flickr.co...ffpottery/sets/
CWU offers; BA, BFA, and MFA Degrees, (Post Baccalaureate also available). Images of CWU Ceramics studio can be seen at
http://www.flickr.co...57623735313670/
Head of Ceramics, Central Washington University
Ellensburg WA
http://stiffyguss.blogspot.com/
http://liquidceramics.blogspot.com/
http://teapotspitchers.blogspot.com/
http://woodkilns.blogspot.com/
http://jomonhaniwa.blogspot.com/
http://stephensrobison.blogspot.com/
http://www.flickr.co...ffpottery/sets/
CWU offers; BA, BFA, and MFA Degrees, (Post Baccalaureate also available). Images of CWU Ceramics studio can be seen at
http://www.flickr.co...57623735313670/
#4
Posted 11 November 2012 - 05:54 PM
Mark C., on 11 November 2012 - 12:54 AM, said:
A photo would really help in this.
Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??
Mark
Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??
Mark
Here are some photos. It does not appear to have a seem. I am assuming I should replace the lid and bottom with normal kiln bricks.
Thanks for replying so quickly to both who responded
Attached File(s)
-
IMG_20121111_164800.jpg (1.57MB)
Number of downloads: 17 -
IMG_20121111_164928.jpg (1.87MB)
Number of downloads: 27 -
IMG_20121111_164837.jpg (2.24MB)
Number of downloads: 23 -
IMG_20121111_165023.jpg (1.49MB)
Number of downloads: 12
#5
Posted 11 November 2012 - 06:59 PM
That is ceramic fiber-do not breath the fibers-looks like your lid had a layer glued to it and the floor looks cracked and they put down a layer of fiber-you will need to remove fiber and replace bricks-the lid looks like it has a huge fallout problem onto stuff.You can also just but a new lid and floor as well.
Mark
Mark
Mark Cortright
www.liscomhillpottery.com
www.liscomhillpottery.com
#6
Posted 11 November 2012 - 08:29 PM
Mark C., on 11 November 2012 - 06:59 PM, said:
That is ceramic fiber-do not breath the fibers-looks like your lid had a layer glued to it and the floor looks cracked and they put down a layer of fiber-you will need to remove fiber and replace bricks-the lid looks like it has a huge fallout problem onto stuff.You can also just but a new lid and floor as well.
Mark
Mark
Ok thank you so much for your help!
#7
Posted 12 November 2012 - 09:30 AM
I've replaced this type of floor and lid on several Duncan kilns with a typical brick floor/lid. These fiber modules were terribly weak and crumbly.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com
neil@neilestrickgallery.com
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com
neil@neilestrickgallery.com
Page 1 of 1

Sign In
Register
Help









MultiQuote