: Duncan Kiln 1029 -strange material lid and floor -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Duncan Kiln 1029 -strange material lid and floor

#1 User is offline   HeatherT Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 10-November 12

Posted 10 November 2012 - 09:04 PM

Hello,

I just bought a Duncan 1029-2. The bricks seem to be in good shape other than the lid and the floor. They seem to be made of some other material than the usual brick used in kilns and I have never seen anything like it. It seems to be disintegrating and looks similar to a fiber blanket material. Does anyone know what it is? Does anyone know if replacing the lid and the floor with regular kiln brick will work?

Thank you for your help!
Heather
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 11 November 2012 - 12:54 AM

A photo would really help in this.
Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   Stephen Robison Icon

  • Moderator
  • Icon
  • Group: Moderators
  • Posts: 132
  • Joined: 29-March 10

Posted 11 November 2012 - 05:14 PM

Get some insulating fire brick, (soft bricks), and replace the floor and lid, that should work fine.
STEPHEN ROBISON
Head of Ceramics, Central Washington University
Ellensburg WA

http://stiffyguss.blogspot.com/
http://liquidceramics.blogspot.com/
http://teapotspitchers.blogspot.com/
http://woodkilns.blogspot.com/
http://jomonhaniwa.blogspot.com/
http://stephensrobison.blogspot.com/
http://www.flickr.co...ffpottery/sets/

CWU offers; BA, BFA, and MFA Degrees, (Post Baccalaureate also available). Images of CWU Ceramics studio can be seen at

http://www.flickr.co...57623735313670/
0

#4 User is offline   HeatherT Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 10-November 12

Posted 11 November 2012 - 05:54 PM

View PostMark C., on 11 November 2012 - 12:54 AM, said:

A photo would really help in this.
Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??
Mark



Here are some photos. It does not appear to have a seem. I am assuming I should replace the lid and bottom with normal kiln bricks.

Thanks for replying so quickly to both who responded :)

Attached File(s)


0

#5 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 11 November 2012 - 06:59 PM

That is ceramic fiber-do not breath the fibers-looks like your lid had a layer glued to it and the floor looks cracked and they put down a layer of fiber-you will need to remove fiber and replace bricks-the lid looks like it has a huge fallout problem onto stuff.You can also just but a new lid and floor as well.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#6 User is offline   HeatherT Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 10-November 12

Posted 11 November 2012 - 08:29 PM

View PostMark C., on 11 November 2012 - 06:59 PM, said:

That is ceramic fiber-do not breath the fibers-looks like your lid had a layer glued to it and the floor looks cracked and they put down a layer of fiber-you will need to remove fiber and replace bricks-the lid looks like it has a huge fallout problem onto stuff.You can also just but a new lid and floor as well.
Mark


Ok thank you so much for your help!
0

#7 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,239
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 12 November 2012 - 09:30 AM

I've replaced this type of floor and lid on several Duncan kilns with a typical brick floor/lid. These fiber modules were terribly weak and crumbly.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com