Does anyone have an idea how to avoid clays that have to sit for a long time in buckets. I have of course covered the buckets. i have tried lavender. But some clays really develop an awful smell i no time at all.
0

#2 User is offline   AndyL Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 93
  • Joined: 31-March 10
  • LocationNJ, USA

Posted 20 July 2010 - 10:41 AM

Add some hydrogen peroxide to your buckets.
0

#3 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,450
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 20 July 2010 - 05:12 PM

I have used a few drops of bleach.
Marcia Selsor
0

#4 User is offline   nepheline Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 9
  • Joined: 19-July 10

Posted 21 July 2010 - 01:59 AM

View PostMarcia Selsor, on 20 July 2010 - 11:12 PM, said:

I have used a few drops of bleach.


Thank you Marcia. I have tried bleach. It works a couple of days but then the smell takes over. The idea is to let the clays sit as long as the buckets are not full. When they are full, I spend half a day dealing with all the clays that need to be recycled. Otherwise I spend too much time and use too much space dealing with small amounts of used clays. The problem is particularly strong with porcelain and very fine stoneware (without grog.)
0

#5 User is offline   nepheline Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 9
  • Joined: 19-July 10

Posted 21 July 2010 - 02:02 AM

View PostAndyL, on 20 July 2010 - 04:41 PM, said:

Add some hydrogen peroxide to your buckets.




Thank you Andy. I know nothing about hydrogen peroxide. Can you tell me an approximate percentage ? Does it alter in any way the quality of the clay ? Does it require wearing gloves ?


0

#6 User is offline   AndyL Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 93
  • Joined: 31-March 10
  • LocationNJ, USA

Posted 21 July 2010 - 10:09 AM

View Postnepheline, on 21 July 2010 - 03:02 AM, said:

View PostAndyL, on 20 July 2010 - 04:41 PM, said:

Add some hydrogen peroxide to your buckets.




Thank you Andy. I know nothing about hydrogen peroxide. Can you tell me an approximate percentage ? Does it alter in any way the quality of the clay ? Does it require wearing gloves ?


Hydrogen Peroxide doesn't affect my clay nepheline. I go more by feel then percentage when I add it. Start at 2 tablespoons in your bucket. BTW you didn't mention the size of your buckets These are 5 gallon ones?
0

#7 User is offline   nepheline Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 9
  • Joined: 19-July 10

Posted 21 July 2010 - 12:33 PM

On my side of the world, gallons are liters... but yes my buckets are - if I count right - approximately 5 gallons.
0

#8 User is offline   AndyL Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 93
  • Joined: 31-March 10
  • LocationNJ, USA

Posted 21 July 2010 - 12:40 PM

View Postnepheline, on 21 July 2010 - 01:33 PM, said:

On my side of the world, gallons are liters... but yes my buckets are - if I count right - approximately 5 gallons.



Ok, There shouldn't be a problem then with 2 tablespoons. Keep in mind like the bleach you'll need to add more from time to time.
0

#9 User is offline   nepheline Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 9
  • Joined: 19-July 10

Posted 22 July 2010 - 12:55 AM

View PostAndyL, on 21 July 2010 - 06:40 PM, said:

View Postnepheline, on 21 July 2010 - 01:33 PM, said:

On my side of the world, gallons are liters... but yes my buckets are - if I count right - approximately 5 gallons.



Ok, There shouldn't be a problem then with 2 tablespoons. Keep in mind like the bleach you'll need to add more from time to time.


Thanks. Will try!