Marcia Selsor, on 20 July 2010 - 11:12 PM, said:
I have used a few drops of bleach.
Thank you Marcia. I have tried bleach. It works a couple of days but then the smell takes over. The idea is to let the clays sit as long as the buckets are not full. When they are full, I spend half a day dealing with all the clays that need to be recycled. Otherwise I spend too much time and use too much space dealing with small amounts of used clays. The problem is particularly strong with porcelain and very fine stoneware (without grog.)