Another glaze I mixed up today was some
old MS34 Burnt Sienna. (2 kg dry)
I'm guessing that this is a Luguna product.
I mixed up the powdered glaze with a high speed blender for 5 minutes and transferred to another bucket through a sieve.
The amount of solids in the sieve was startling.
There was enough material in the sieve (maybe 500 - 600 grams) that I figure that it should be either in solution or a
much finer particle in suspension.
Has anyone seen this occur with old glazes or this burnt sienna?
I put all of it back into the bucket and mixed another 5 minutes.
I will allow it to hydrate overnight and give it another mix in the morning.