We fire pottery in wood kilns in Taiwan. one of the wood kilns we built reached to 1516 degree Celsius days ago. The temperature set up the highest record of wood kiln so far in Taiwan. We would like to know the highest record for wood kilns in the world.
Thanks a lot.
#2
Posted 05 November 2012 - 01:41 AM
Mei, on 04 November 2012 - 09:00 AM, said:
We fire pottery in wood kilns in Taiwan. one of the wood kilns we built reached to 1516 degree Celsius days ago. The temperature set up the highest record of wood kiln so far in Taiwan. We would like to know the highest record for wood kilns in the world.
Thanks a lot.
what cone did you guys actually have down? Was that just a momentary measurement on a pyrometer? I think the highest I've seen was cone 15 down in the front of a train kiln--it was a mess.
#3
Posted 05 November 2012 - 09:26 AM
Many people in the USA are using pyrometers with type K thermocouples... because they are cheap..... so I would take any readings you hear from folks here with a bit of "a grain of salt" (meaning not necessarily all that accurate) because above about 2350 F the readings become unreliable and over time there is significant drift in their accuracy. If they are not uising Type S thermocouples.... the number thay have is kind of meaningless in a "competition" kind of situation.
best,
........................john
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art
http://www.JohnBaymore.com
#4
Posted 06 November 2012 - 08:54 AM
This is Derek from Taiwan. The kiln that had reached 1516℃was built by my master, Mr. Lin. As he doesn't speak English, I am here to respond for him.
Mr. Lin uses type R thermocouples as there’s only type K and R in Taiwan.He haven’t used any cone for over 10 years as he tried type R thermocouples,cone 16, PCTR, and Infrared thermometer once in his horizontal wood firing kiln ten years ago. The cone melted into liquid, and both TCPC and Infrared thermometer indicated over 1500℃when the peak pyrometer read 1447℃ with type R thermocouples. He took the pyrometer reading and decided not to use cone ever since. In his way of firing in the last 10 years, he always reaches peak at between 1380-1420℃ and maintain the temperature over 1300℃over 12 hours.
This very kiln that hit 1516℃is a downdraft style wood firing kiln built by him in May, 2012. Within the 54-hour burning process, temperature was remained over 1400℃over 12 hours, and we hit temperature over 1500℃ over five times in 8 hours.
He will open the kiln this Saturday and we will post the picture to share with everybody ASAP.
Sincerely,
…………Derek Chuang
#5
Posted 06 November 2012 - 09:35 AM
Derek1229, on 06 November 2012 - 08:54 AM, said:
Derek,
Yes, Please!
best,
......................john
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art
http://www.JohnBaymore.com
#6
Posted 13 November 2012 - 11:28 AM
Sorry for waiting. It take some time editing and correcting this film. Hope you like it!
http://www.youtube.c...ukNyGSfOx4&hd=1
Sincerely,
...................Derek
#7
Posted 13 November 2012 - 11:57 AM
interesting that you use the same method of filling the front with wood and just letting the fire draw it in, here we call that the wood-pig. often we fill up the opening top to bottom flush with the front wall, then close the door for a few seconds, then open and gently push all the wood in and repeat...that will get it going!
#8
Posted 13 November 2012 - 08:06 PM
Cass, on 14 November 2012 - 12:57 AM, said:
That's the feldspar pellets (a type of mineral used as flux) aswell as some silicon contained in the primary clay that Mr. Lin used in his works. During the high temperature, some finer clay in primary clay would melt and transformed into glaze and the little stones would rather melted into white spots or remain there. That's where the white coarse came from.
Sincerely.
........Derek
#9
Posted 13 November 2012 - 09:41 PM
#11
Posted 14 November 2012 - 04:56 PM
John
#12
Posted 14 November 2012 - 08:22 PM
JLowes, on 15 November 2012 - 05:56 AM, said:
John
Thank you, John. We've been searching for his info for days.
Sincerely.
..................Derek

Sign In
Register
Help










MultiQuote