Fresh clay Too soft for throwing - suggestions? Rate Topic: -----

#1 User is offline   Nancy S. Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 62
  • Joined: 05-September 12

Posted 03 November 2012 - 05:13 PM

This may well be in the archives, but the search function isn't working and I'm too impatient to wait. ;)

I have a brand-new 25-pound bag of clay, and it's incredibly soft (in spite of sitting around for at least four months!) - unfortunately it's a bit too soft for throwing anything more than a 1/2-pound at a time without collapsing. I tried kneading the clay on an absorbent surface first, but it wasn't enough.

What's the best way to dry out the clay enough to throw? I don't want it to get too dry...I don't have a pugmill, so reclaiming is a long and arduous process. Any suggestions are appreciated!!

0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,436
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 03 November 2012 - 05:32 PM

divide it up into quarters the long way, round it out into rolls and stand them up in horse shoe shapes to dry out a bit.
Than wedge them up.

Marcia
Marcia Selsor
0

#3 User is offline   Nancy S. Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 62
  • Joined: 05-September 12

Posted 03 November 2012 - 06:43 PM

View PostMarcia Selsor, on 03 November 2012 - 06:32 PM, said:

divide it up into quarters the long way, round it out into rolls and stand them up in horse shoe shapes to dry out a bit.
Than wedge them up.

Marcia


I will try that! Thanks so much!!