#21 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 25 October 2012 - 12:42 PM

View Postclay lover, on 24 October 2012 - 03:27 PM, said:

Lucille, if you have Clorox in all the wet things in your studio, doesn't it eat your hands after a day of working in it?

I, too, like the clean smell, but worry about skin effects. with daily use.



I don't throw every day. But when I do, I only use the amount recommended by Clorox to kill the bacteria. I never put so much bleach in the water that I can smell it. I know bleach can be 'lethal' so I went to the Clorox web site and found out how much to use.