: Converting FFF feldspar -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Converting FFF feldspar

#1 User is offline   Jan jones Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 13-October 12
  • LocationPerth, Western Australia

Posted 13 October 2012 - 12:43 AM

Does anyone know what proportions of potash feldspar and nephelline syenite can be used to replace FFF feldspar in a glaze recipe. FFF feldspar does not seem to be available in Australia?
0

#2 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,484
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 13 October 2012 - 09:29 AM

Can you post the typical analysis of the FFF feldspar you mention? If you do, I can recalculate it using other materials.

But to really be accurate I would also need the typical analysis of your OTHER raw materials that might be used to substitute..... the Neph. SY. and so on.

best,

.......................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#3 User is offline   Jan jones Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 13-October 12
  • LocationPerth, Western Australia

Posted 13 October 2012 - 10:27 PM

View PostJBaymore, on 13 October 2012 - 09:29 AM, said:

Can you post the typical analysis of the FFF feldspar you mention? If you do, I can recalculate it using other materials.

But to really be accurate I would also need the typical analysis of your OTHER raw materials that might be used to substitute..... the Neph. SY. and so on.

best,

.......................john

Thanks so much for the offer of help, I am a new hobby potter and using the lovely new book from Linda Bloomfield called : Colour in glazes, I do not have the precise composition of my materials from my supplier but, Am happy to test, test test.


The FFF FELDSPAR IS: SiO2 67.7, Al2O3 18.9, , Fe2O3 0.16, CaO 0.72, K2O 7.62, Na2o 4.84 LOI 0.05.

The Potash Feldspar is: SiO2 65.8, Al2O3 18.5, Fe2O3 0.1, CaO 0.38, K2O 12, Na2o 2.89, LOI 0.33

The Nephaline Syenite is: SiO2 60.5, Al2O3 23 , Fe2O3 0.1, CaO 1, K2O 1, Na2o 10.2 , LOI 0.2

I also have a problem with the rutile pink glaze from the book, , come , 8 oxidised, but is firing clear. the recipe is:

Any hints gratefully received.

Nephelline Syenite. 26
Whiting. 12
Lithium carb. 10
Barium carb. 3
Calcium borate fruit. 5
Quartz. , 44

+

Rutile. 1.5
Tin oxide. 4

Kind regards

Jan
0

#4 User is offline   ayjay Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 99
  • Joined: 05-November 11

Posted 14 October 2012 - 10:45 AM

View PostJan jones, on 14 October 2012 - 04:27 AM, said:

Calcium borate fruit. 5


Jan


That'll be the 5 portions for the day then. :D ;)
0

#5 User is offline   Jan jones Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 3
  • Joined: 13-October 12
  • LocationPerth, Western Australia

Posted 14 October 2012 - 07:28 PM

View Postayjay, on 14 October 2012 - 10:45 AM, said:

View PostJan jones, on 14 October 2012 - 04:27 AM, said:

Calcium borate fruit. 5


Jan


That'll be the 5 portions for the day then. :D ;)