#1 User is offline   Wind n Wing Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 56
  • Joined: 21-April 11

Posted 11 October 2012 - 12:29 PM

I have replaced all the elements in my small Duncan. In the process a section of kiln brick about 4" came off and the element is exposed. It wants to buldge. I have watched the video on Paragons site to see how to use pins/staples to keep it in place. It appears that it is alright if the pins touch the element itself. But before I insert the pins I want to make sure I am seeing things correctly. So will there be any electrical problems if the pins touch the element. Dont want to waste time and effort by not measuring twice and cutting oncePosted Image as the old adage goes.

Thanks
RJ
0

#2 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,191
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 11 October 2012 - 01:12 PM

The pins are intended to touch the elements. The pin should be placed in between two of the loops, holding the element down at the bottom of the loop. You can also support a sagging coil by putting the pin at the top of the loop, with the element essentially hanging on the pin. The chunk of brick can be put back into place with pins, too, as a temporary fix until you can replace the brick. If the chunk is so large that the element can sag out of its groove, the brick should be replaced. Do it now when you are doing the elements.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#3 User is offline   Wind n Wing Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 56
  • Joined: 21-April 11

Posted 11 October 2012 - 07:11 PM

View Postneilestrick, on 11 October 2012 - 11:12 AM, said:

The pins are intended to touch the elements. The pin should be placed in between two of the loops, holding the element down at the bottom of the loop. You can also support a sagging coil by putting the pin at the top of the loop, with the element essentially hanging on the pin. The chunk of brick can be put back into place with pins, too, as a temporary fix until you can replace the brick. If the chunk is so large that the element can sag out of its groove, the brick should be replaced. Do it now when you are doing the elements.


Thanks Neil,

I have pinned the pieces of brick and things look pretty good. Everything is in place and ready to go.

RJ