Glaze Inside To Strenghten Eartenware? Rate Topic: -----

#1 User is offline   Lucy Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 25
  • Joined: 31-March 10

Posted 11 July 2010 - 03:08 PM

I am making some ^05 earthenware sculptures that have potentially fragile appendages and joints. (I'll eventually be using cold finishes on the outside.) Would glazing the inside improve their strength?
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,453
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 15 July 2010 - 03:12 PM

I think I'd ad fiber to the clay rather than count on a glass coating a few mm thick. Glaze is not really a structural element.it is a very thin coating. Maybe it would be better than nothing, but you could run into problems of surface tension with only one side (inside) having glaze on it.