Hey world,

I am loading a kiln for a bottle slumping and I forgot what cone to fire to, I think it might be ^012? Please help!
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit
0

#2 User is online   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 28 September 2012 - 02:34 PM

Glass slumps at very low temps-I about 37 years ago tried to fire my own labels on beer bottles and all the necks slumped as well-So if memory serves its way below luster temps.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   Idaho Potter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 316
  • Joined: 26-August 10
  • LocationBoise, Idaho

Posted 28 September 2012 - 04:20 PM

Google "slumping temperature of glass" you'll find many choices. I occasionally use glass threads, etc on some pots (decorative) and needed some help with temps. Started using a blog called "HOT OUT OF THE KILN'. They have a monthly newsletter as well. Might find it helpful.
0

#4 User is offline   giltex58 Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 45
  • Joined: 03-August 11
  • LocationGilmer, Texas

Posted 28 September 2012 - 08:02 PM

View PostIforgot, on 27 September 2012 - 08:48 PM, said:

Hey world,

I am loading a kiln for a bottle slumping and I forgot what cone to fire to, I think it might be ^012? Please help!


I do quite a bit of slumping. Just checked my firing log. Cone 015 with a 15 minute hold after a "fast" firing schedule. I just leave the kiln alone till it cools down to about 100