What Is This And This and this? and that and that ?

#1 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 06 September 2012 - 04:01 AM

This is a five fold 'quiz'. What is it and what does it represent and what is it made from and what is the glaze, and what is its country of origin? Some of the answers are easy, others not too much. No screen shots.


Attached File  an image.jpg (14.29K)
Number of downloads: 242

INRI
0

#2 User is online   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,429
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 06 September 2012 - 07:48 AM

Wow Lucille, that is a stumper. A side view might help. The glaze is a beauty.
Nice carving. I am leaving for Europe today for a residency in France. I will try to check back to see the answer!
Marcia
Marcia Selsor
0

#3 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,359
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 06 September 2012 - 10:36 AM

I'll take a shot at the clay body being porcelain and the glaze being a Celadon.
No idea what it is but those holes look like vents so maybe a candle holder of some type?
Good one!
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#4 User is online   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,429
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 06 September 2012 - 12:29 PM

Is it an inhaler? Chinese?
marcia
Marcia Selsor
0

#5 User is offline   LawPots Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 45
  • Joined: 11-April 11

Posted 06 September 2012 - 03:12 PM

My guess is Celedon glaze, Korean-made, light-colored stoneware, and, while I almost can't believe I'm going to write this, it looks like a ceremonial hat :)


0

#6 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 695
  • Joined: 07-December 11
  • LocationCanada

Posted 06 September 2012 - 03:37 PM

My first thought was that it was a piece by Richard Zakin, then I saw the carving.
The clay is porcelain, carved, then glazed with a Celadon glaze. It is some kind of strainer or funnel, and is upside down when in use.
What do I win?
Tom[TJR].
0

#7 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 07 September 2012 - 05:41 PM

There were many correct answers; we are getting there. Here are some of the answers.

1.
2. Porcelain
3. Celadon
4. a hat (courtier's cap)
5.
And as per Marcia's request.

Attached File  #2 image.jpg (16.25K)
Number of downloads: 122

Lawpots, that was a very good observation.
TJR there is no prize per se it is just the joy of being correct.

INRI
0

#8 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 695
  • Joined: 07-December 11
  • LocationCanada

Posted 07 September 2012 - 07:44 PM

View PostLucille Oka, on 07 September 2012 - 05:41 PM, said:

There were many correct answers; we are getting there. Here are some of the answers.

1.
2. Porcelain
3. Celadon
4. a hat (courtier's cap)
5.
And as per Marcia's request.

Attachment #2 image.jpg

Lawpots, that was a very good observation.
TJR there is no prize per se it is just the joy of being correct.


I know there is no prize other than the joy of being corrent. I was just being facetious.Thank-you for posting.
Tom[TJR]
0

#9 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 07 September 2012 - 08:38 PM

View PostTJR, on 07 September 2012 - 04:44 PM, said:

I know there is no prize other than the joy of being corrent. I was just being facetious.Thank-you for posting.
Tom[TJR]



I know you were. One of the worse things about social media is not being able to hear the inflections in the voices. Smiley faces just don't show it well enough.
INRI
0

#10 User is online   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,429
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 08 September 2012 - 12:37 AM

thanks for the side view. It reminds me of some of those strange ceramic medical devices I saw at the Medical Museum in Switzerland.
Not Chinese with such carving with a celadon, then maybe Korean?
Is it a hat that one would put flowers in like a Dutch tulip holder?
The courtier would be decorated with flowers?
arcia
Marcia Selsor
0

#11 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 08 September 2012 - 01:13 AM

As a medical device it would scare me.
INRI
0

#12 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 09 September 2012 - 06:33 AM

Ok, the place of origin is Japan. One answer left and I am holding off for the one last answer. A hint: Chris was the closest.
So you must keep thinking about it. Even though this vessel is almost 400 years old its use can still be employed today.

INRI
0

#13 User is offline   Mossyrock Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 135
  • Joined: 22-August 10
  • LocationHigh Point, NC

Posted 09 September 2012 - 12:51 PM

Possibly an incense burner?
Brenda Moore
Mossy Rock Creations
High Point, NC
0

#14 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 09 September 2012 - 03:09 PM

View PostMossyrock, on 09 September 2012 - 09:51 AM, said:

Possibly an incense burner?



Yes, it is an Incense Burner in the shape of a Courtier's cap with peonies. It is made of a Porcelain body and a celadon glaze. Japan 1690. Bravo!


INRI
0

#15 User is offline   agatha.gao Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 14
  • Joined: 02-December 12

Posted 02 December 2012 - 10:26 AM

this is an antique carved lotus pattern with celadon from Song Dynasty.