: kiln to use laid on the side -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

kiln to use laid on the side 45 degree volt kiln? Rate Topic: -----

#1 User is offline   claclana Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 55
  • Joined: 17-April 11
  • LocationBuffalo, NY

Posted 04 September 2012 - 07:08 PM

Hello
I could put my hands on a bigger electrical kiln (inside 17"x 24") , but I need wider more than taller...


is it too crazy to use it laid on the side? Posted Image
may be with some external support for the walls and a fake floating floor...did anyone have done it?
Thanks!
0

#2 User is offline   neilestrick Icon

  • Neil Estrick
  • PipPipPip
  • Group: Members
  • Posts: 1,240
  • Joined: 04-October 11
  • LocationGrayslake, IL

Posted 04 September 2012 - 08:14 PM

From a liability standpoint, no one here should say yes to that. From a practical standpoint, the bricks will probably crumble, and it'd be near impossible to get any shelves in there since the 'floor' would be curved and covered with elements.
Neil Estrick
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com
0

#3 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 739
  • Joined: 07-December 11
  • LocationCanada

Posted 04 September 2012 - 08:47 PM

I agree with Neil. This sounds dicey. I would look for a used square or oval kiln. I don't think kilns are designed to be on their sides.
TJR.
0

#4 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 04 September 2012 - 11:08 PM

Really bad idea.
Mark
Mark Cortright
www.liscomhillpottery.com
0

#5 User is offline   claclana Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 55
  • Joined: 17-April 11
  • LocationBuffalo, NY

Posted 05 September 2012 - 05:00 PM

OK!...
ditched the idea!
THANKS!
0