Posted 02 September 2012 - 12:26 PM

I'm slip-casting hundreds of 4" circles (pot feet) in one piece plaster molds. Each one is a little different, and that's ok, but they come out with a sharp, irregular lip, as that lip forms at the top of the pour. I need to simply shape or easy these lips, lots of em. I'm willing to build any sort of jig or tool to do this. Suggestions?

R
0

#2 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,360
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 02 September 2012 - 02:06 PM

You could sand them on a large sanding disc that attaches to a power wheel head when they are at the right moisture content. You could use a sure form then sponge you could use a power sponge after cutting them (this is a 500$ tool)
You could chuck them on power wheel and trim lips(fastest way I think)



All this takes time I suggest in the long run making a better mold ( a two piece with the rim/lip as the top with a hole in to dump out the slip)that makes the rim smooth from the start.Happy trimming-
Mark
Mark Cortright
www.liscomhillpottery.com
0

#3 User is offline   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,360
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 02 September 2012 - 08:39 PM

ops
Mark Cortright
www.liscomhillpottery.com
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users