Fall sunny weather is upon us and the sun still has some drying to it so I put the am production in sun to quick dry it. most of this was no trimmers. I used about a 1/3 of this in load- this afternoon-the mugs without handles will get bisqued in AM after handles go on and sit the night covered.
The sun is your friend in the right climate this time of year.
Mark