: How to get raised designs? -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

How to get raised designs? Rate Topic: -----

#1 User is offline   nancylee Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 100
  • Joined: 21-May 11
  • LocationUpstate NY

Posted 21 August 2012 - 06:09 AM

Hi all,
I am looking to make some smaller things for the holidays and buttons. How do you get raised images on your buttons? I am thinking of face buttons, or animals, etc, raised on the surface.

I know how to carve into the clay, but buttons and earrings are so small, are molds used? And if so, where might one buy molds for pottery, or where would I learn to make molds. I am NOT a good draftsman, have trouble drawing realistically.
Thanks,
Nancy
Nancy
Northern Woods Pottery
www.northernwoodsstudio.blogspot.com
0

#2 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,430
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 21 August 2012 - 06:43 AM

Nancy,
You could use bisque molds. Carve a negative and bisque it OR make a positive, bisque it then, press clay around it and bisque that. You would probably get around 5% shrinkage each time. Clay press molds have been used for 1000s of years. If you want a nice clean mold you could make the positives out of an oil based clay,
cast that in plaster. Then you could press mold with that.
Marcia Selsor
0

#3 User is offline   nancylee Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 100
  • Joined: 21-May 11
  • LocationUpstate NY

Posted 21 August 2012 - 06:47 AM

View PostMarcia Selsor, on 21 August 2012 - 06:43 AM, said:

Nancy,
You could use bisque molds. Carve a negative and bisque it OR make a positive, bisque it then, press clay around it and bisque that. You would probably get around 5% shrinkage each time. Clay press molds have been used for 1000s of years. If you want a nice clean mold you could make the positives out of an oil based clay,
cast that in plaster. Then you could press mold with that.



Hi Marcia,
Thank you! I have never even heard of a oil based clay!! I found some molds, silicon ones, can they be used with the clay we use? Most say polymer clay.
Thanks again,
Nancy


Nancy
Northern Woods Pottery
www.northernwoodsstudio.blogspot.com
0

#4 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,362
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 21 August 2012 - 10:31 AM

If all you want to do is press a bit of clay into a mold to get a design, you can use just about any kind of mold ... I would recommend searching your local crafts store ... Like a Michael's ... see what they have in the clay, cake, candy, scrap booking, woodworking areas. Just press the clay in and use another piece of clay to pull it out.
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#5 User is offline   dave the potter Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 20
  • Joined: 17-November 10

Posted 21 August 2012 - 11:07 AM

Having a spray can of PAM around is a good idea. Items that do not release easily, whether positives you are using to make molds or molds for other materials i.e. polymer clay, will work just fine after a light spray.
0

#6 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 695
  • Joined: 07-December 11
  • LocationCanada

Posted 21 August 2012 - 03:12 PM

You can use plastecine, which is an oil based clay. Make your small buttons and then make a plaster mold of a group of them.
TJR.
0

#7 User is offline   Seasoned Warrior Icon

  • Businessman - Potter
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 294
  • Joined: 02-April 10

Posted 21 August 2012 - 03:36 PM

View Postnancylee, on 21 August 2012 - 04:09 AM, said:

Hi all,
I am looking to make some smaller things for the holidays and buttons. How do you get raised images on your buttons? I am thinking of face buttons, or animals, etc, raised on the surface.

I know how to carve into the clay, but buttons and earrings are so small, are molds used? And if so, where might one buy molds for pottery, or where would I learn to make molds. I am NOT a good draftsman, have trouble drawing realistically.
Thanks,
Nancy


Marcia's recommendations are spot on as usual. Oil clay is modelling clay which many potters refer to using a trademarked name such as Plasticine. Bisque molds if you are not familiar with making plaster molds are quite easy just press what yo want into a piece of clay, bisque it and voila! (a tip of the hat to Marcia's upcoming residence) you have a negative cavity that will produce many copies by pressing balls of clay into the cavities. One of the ways to get good impressions and constant density is to make a wooden press kind of like a tortilla press. Make little balls of clay and press them into either your bisque or plaster molds. Just make a little channel around the cavity for excess clay to extrude into. You can make an incredible variety and quantity of tiny items with this very simple setup.