Posted 20 August 2012 - 03:00 PM

Yay Me! :) I just ran my kiln for the very first time, all by myself, and it worked. Those of you who have been doing this forever are thinking, "so what?", but I am very excited! I wasn't sure if I would be able to figure out the controls, which turned out to be ridiculously easy. We did blow the fuse, but once my husband replaced it with the correct size, we were fine.

Now I have a LOT of glazing to do.
0

#2 User is offline   atanzey Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 106
  • Joined: 02-December 10
  • LocationSouth-Central Pennsylvania

Posted 20 August 2012 - 05:06 PM

Congratulations! I felt the same way when I finished my first firing - and my 'new to me' electric kiln was only a couple of weeks ago!

Alice
0

#3 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,398
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 20 August 2012 - 05:19 PM

Congratulations ... isn't it great!!!
I have been doing this for 25 years and on Sunday I was out in the garage unloading a bisque load that was too hot to touch ... ouch, ouch ouch ... but I kept on going. It never gets old.:D
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#4 User is offline   sawing Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 48
  • Joined: 06-June 12
  • LocationAnn Arbor, MI

Posted 20 August 2012 - 05:51 PM

My kiln is "new to me", too, and I was apprehensive that it wouldn't work. I didn't pay much for it. It's good to know that this feeling doesn't go away, and that I can look forward to this every time I fire. Gotta go glaze!
0

#5 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,494
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 20 August 2012 - 06:09 PM

Congratulations...now you have to glaze and fire!!
It's the beginning of the never ending cycle!
Marcia
Marcia Selsor
0

#6 User is offline   yedrow Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 367
  • Joined: 06-February 12

Posted 20 August 2012 - 07:56 PM

Congratulations. Every success in a world so mysterious as fire and earth is a wonderful. With every mastered skill comes something else that is strange and intriguing.
0

#7 User is offline   sawing Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 48
  • Joined: 06-June 12
  • LocationAnn Arbor, MI

Posted 20 August 2012 - 08:44 PM

View Postyedrow, on 20 August 2012 - 08:56 PM, said:

With every mastered skill comes something else that is strange and intriguing.


My family thinks this whole process is strange and intriguing. They stand around watching me throw, trim, load and unload the kiln as though it was a spectator sport. :)
0

#8 User is offline   Mark McCombs Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 111
  • Joined: 13-August 12
  • LocationSW Washington

Posted 20 August 2012 - 11:37 PM

Congratulation, Sawing. It is a big deal. :lol: My first bisque firing was a few weeks ago. It was really neat. I have had two glaze firing since.

Be sure to double check your wire size from the panel/fuse box to the kiln to insure the correct wire size if you are going to fire at a higher cone later on.
Don't need a power failure during glaze fire.


B)
Mark
Fast Hawk Pottery


^5-6 Ox
1227 Skutt
0

#9 User is offline   Jime Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 20
  • Joined: 02-October 12

Posted 22 October 2012 - 09:33 PM

I just ran into this old thread, and I was happy to hear there are other firing newbs around!!
I just got a kiln, and will be taking on my first firing in a few months. Glad to know there are others around trying to figure stuff out, it makes it a little less intimidating!
0

#10 User is online   Brian Reed Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 108
  • Joined: 14-August 12
  • LocationWashington State

Posted 22 October 2012 - 11:22 PM

That is just great, in fact I am in the same boat as you. I recently fired my first bisque kiln and now I have done 4 bisque fires in my electric. Two weeks ago I did my first galze fire with my gas kiln to ^10 reduction and it also worked great. I had issues with the high fire, but I know what I did wrong and learned what not to do next.



Keep it up and keep us informed we can all learn together.
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club
0

#11 User is offline   Sylvia Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 15-June 12

Posted 23 October 2012 - 05:23 PM

I'm doing my first bisque firing this weekend
I'm so glad to hear that all of you are having success
0

#12 User is offline   Jime Icon

  • Member
  • PipPip
  • Group: Members
  • Posts: 20
  • Joined: 02-October 12

Posted 25 October 2012 - 10:11 PM

yay Sylvia!!
I'll be rooting for you!
let us know how it goes!
0

#13 User is offline   SmartsyArtsy Icon

  • Chris Seminara
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 148
  • Joined: 29-October 11
  • LocationPNW

Posted 27 October 2012 - 12:50 AM

Excited for you; The glaze firing will continue to be a thrill. It's difficult but important not to rush the unveilings (opening the kiln). Enjoy!


Chris
Chris Seminara Ceramics
Member, Artisan Tile NorthWest
0

#14 User is offline   sawing Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 48
  • Joined: 06-June 12
  • LocationAnn Arbor, MI

Posted 28 October 2012 - 08:53 AM

Since someone else resurrected this thread, I will update. I have since fired another bisque and two glaze. It's exciting and disappointing to see the successes and failures, but I learn something each time. I have actually sold a couple of pieces; spoon rests, sponge holders, yarn bowls... nothing too brilliant, but still encouraging!

On the downside, I have been working a LOT, and have not had any time at all in my studio lately. I gotta fix that.
0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users