Posted 27 July 2012 - 04:43 AM

I have a Skutt 614 kiln and just finished running a cone 04 bisque fire. Under the element, there is a small amount of black dust. Does this mean my element is burning out? This kiln is new and has only been run a handful of times. Thanks for your help.
0

#2 User is offline   Lucille Oka Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 756
  • Joined: 02-July 10

Posted 27 July 2012 - 07:26 AM

No it doesn't mean that. The elements are oxidizing and the oxidation flakes off into the kiln. It just means you have to vacuum out the grooves so that the flakes won't land in your ware. Since this is a new kiln, look in the kiln manual under ‘maintenance’ and Skutt will show you how to do this. You can also go to the Skutt website and see a video on how to maintain your kiln.


INRI
1

#3 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,445
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 27 July 2012 - 08:12 AM

Good point. It is a good maintenance practice to vacuum your kilns every so often.
I put kiln wash on the cone holder too.
Marcia
Marcia Selsor
0

#4 User is offline   Jaimeta Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 2
  • Joined: 16-July 12
  • LocationEasley, SC

Posted 27 July 2012 - 08:47 AM

Thank you all!