: Nan bread oven -

Jump to content

Share Topic:   facebook stumbleupon del-icio-us digg email google mixx reddit
Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

Nan bread oven

#1 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,436
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 03 July 2012 - 09:49 AM

Attached File  UzbekBukharabreadoven2.jpg (27.17K)
Number of downloads: 79here is a Nan bread over in use. It is a simple teardrop shaped pot with a fire in the bottom that heats up the walls.
I was treated to this bread after a night train from Tashkent to Bukhara. Several of us stayed at my friend's house there. We arrived about 6 am. His mother was baking the bread in the courtyard as we arrived to the house. The bread drops off when it is cooked. She made a big stack for us. It was delicious.

Attached File  Uzbekbreadovn.jpg (24.94K)
Number of downloads: 74

Marcia Selsor
1

#2 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,367
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 03 July 2012 - 10:36 AM

Did you watch the process? I'm assuming she sticks her hand inside each time she has to put one in or out ... so how hot is the oven?
Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
0

#3 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,436
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 03 July 2012 - 11:49 AM

I did watch the process but it was back in 1994 and after riding the night train. I can't remember if she used a tool to pull out the bread to not. I would think some tongs would be better than a bare hand. Obviously it is hot enough to bake bread. It is a very simple oven...and the speed would be similar to a good Italian pizza oven ..about 3 minutes.
She had a stack of no less than 20 of these for about 7 guests and 5 family members.
Marcia
Marcia Selsor
0

#4 User is offline   ~janie Icon

  • ~janie
  • PipPipPip
  • Group: Members
  • Posts: 99
  • Joined: 28-July 10
  • LocationHot old Texas Coast

Posted 03 July 2012 - 12:29 PM

What did the bread taste like? Is it crusty, or soft, like tortillas? I would like to know how to make one of these ovens.
0

#5 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,436
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 03 July 2012 - 12:43 PM

It is Nan as you eat in Indian restaurants. There are tools with pins to poke the center before baking to avoid doughy texture. It is flat bread. Thicker than a tortilla.
Nice crust on the edge and somewhat in the center.

Marcia
Marcia Selsor
0

#6 User is offline   DAY Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 146
  • Joined: 19-January 11

Posted 12 July 2012 - 07:04 PM

View PostMarcia Selsor, on 03 July 2012 - 12:43 PM, said:

It is Nan as you eat in Indian restaurants. There are tools with pins to poke the center before baking to avoid doughy texture. It is flat bread. Thicker than a tortilla.
Nice crust on the edge and somewhat in the center.

Marcia

Many years ago I baked a pizza atop an electric kiln. Used a few stilts and a shelf to make a top to hold in heat.
Has anyone used that "excess" heat to cook? I bet a stew pot could work some magic over a 10 hour firing. . .


0

#7 User is offline   Frederik-W Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 244
  • Joined: 02-January 12
  • Locationa distant moon of Uranus

Posted 13 July 2012 - 11:35 AM

It would be interesting to know how people would see this in different settings,
e.g. 100% purely functional or art if it is put in in e.g. a sculptural garden.

0

Page 1 of 1
  • You cannot start a new topic
  • You cannot reply to this topic

2 User(s) are reading this topic
1 members, 1 guests, 0 anonymous users

  1. ser