Have you experimented working with various clay bodies? | June 25, 2012 Potters Council Question of the Week

#1 User is offline   Carolyn Dorr Icon

  • Administrator
  • Icon
  • View gallery
  • Group: Administrators
  • Posts: 125
  • Joined: 24-February 10
  • LocationColumbus, Ohio

Posted 25 June 2012 - 01:35 PM

Have you experimented working with various clay bodies: stoneware, porcelain, terra cotta, white earthenware? Do you use primarily one body? How did you decide? What are the qualities that made "IT" the one?

Sorry more than one question, but all related... :rolleyes:

I am primarily a stoneware person, but always keep some porcelain nearby. I have wanted for years to use porcelain on a regular basis, but often it is so fraught with problems for the forms I want to make, that I give it a try, and then return to stoneware for its superb flexibility.




Diana Pancioli
Potters Council Board Member
dianamp@comcast.net
dianapancioli.com
Carolyn Dorr
Potters Council
www.potterscouncil.org
0

#2 User is offline   Karen B Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 92
  • Joined: 11-September 10
  • LocationMassachusetts

Posted 29 June 2012 - 12:48 PM

Carolyn, I use 6 clay bodies! That sounds like a lot, but I really need them for different uses.

I use a ^6 speckled stoneware, ^6 porcelain and ^04 terra cotta for throwing similar items with
similar designs. The glazing is so different and I like that variety.

I use a ^04 white earthenware for making detailed 3D decorative tiles.

And a ^6 white stoneware which works better for handbuilding than does porcelain,

Finally I have a very sturdy ^6 clay body which is optimal for permanent outdoor items such as bird baths or flower pots.

I have 2 wheels. One is reserved for dark clay bodies, and the other for white. I am VERY careful about labeling the plastic
bags with a sharpie as they are indiscernible when wet.
0

#3 User is offline   DBCurley Icon

  • Member
  • PipPip
  • View gallery
  • Group: Members
  • Posts: 15
  • Joined: 23-June 12

Posted 30 June 2012 - 10:23 AM

Typically, I've been using three clay bodies as well. For my 1:1 scale humans, I've been using Lisa Clague's brand clay. It's awesome stuff! Super durable, and fires a nice white. For my more masculine forms, I've been using a speckled brown ^6 clay body(I like the glazing effects I can get out of it). And I typically keep about 50lbs of porcelain kicking around when someone wants something in particular like dainty white tea cups.

I've played with some 266 and Red rock recently. I enjoyed them both!
My gallery. please visit!

"A human being should be able to change a diaper, plan an invasion, butcher a hog, conn a ship, design a building, write a sonnet,balance accounts,build a wall, set a bone, comfort the dying,take orders,giveorders,cooperate,act alone, solve equations, analyze a new problem, pitch manure, program a computer, cook a tasty meal, fight efficiently, die gallantly. Specialization is for insects." — Robert Heinlein

'....and throw a mug!' -- Brandon Curley
0

#4 User is offline   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,107
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 01 July 2012 - 09:38 AM

I use B-Mix 5 for my cone 6 pots, Lizella Red for terra cotta/stoneware pots, Frost 5 for cone 6 porcelain, Frost 5 paper clay for cone 6 porcelain, Southern Ice for cone 10 pots, B-Mix woodfire for cone 13 pots, beginning to experiment with clay dug on my land (I live in Lizella which is the namesake of one of the prettiest clays available in the US).

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#5 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,557
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 01 July 2012 - 10:13 AM

View PostOffCenter, on 01 July 2012 - 10:38 AM, said:

(I live in Lizella which is the namesake of one of the prettiest clays available in the US).


You lucky son of a gun! Agree wholeheartedly that Lizella is some great stuff.

best,

.....................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art