Do you have a favorite clay body? | June 12, 2012 Question of the Week | June 12, 2012

#1 User is offline   Deidre Haignere Icon

  • Member
  • Icon
  • Group: Administrators
  • Posts: 17
  • Joined: 27-February 12

Posted 13 June 2012 - 07:33 AM

Do you have a favorite clay body? Stoneware (light or dark), porcelain, terra cotta? Do you work with more than one clay body? Why did you choose the particular clay you use?

I work with two bodies, one that I make and one that I buy. I use stoneware for most of my work, but every now and then I want porcelain for its wonderful qualities (despite its difficulties); I buy it.


Diana Pancioli
Potters Council Board Member
dianamp@comcast.net
dianapancioli.com
0

#2 User is offline   SShirley Icon

  • Cow Creek Pottery
  • PipPipPip
  • Group: Members
  • Posts: 190
  • Joined: 31-March 10
  • LocationPittsburg, Kansas

Posted 13 June 2012 - 08:18 AM

I use a cone 6 porcelain from Flint Hills. It's smooth as butter, really soft (just the way I like it) and I can use it straight from the bag without wedging. I get a thousand pounds at a time and he even delivers it.
0

#3 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,505
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 17 June 2012 - 12:56 AM

I like the terra cotta called Galestra that I use in Tuscany. It is gray wet but fires red. It actually softens the skin when working with it.
It fires to cone 08 and must be soaked with water after firing.
It is a great hand building body and can also be thrown. I believe it comes from Montelupo, outside of Florence.
At home in the US. I make my own terra cotta, raku, and stoneware. I buy porcelain. I like the porcelain I got from Alligator clay in Baton Rouge for ^6

Marcia
Marcia Selsor
0

#4 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,555
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 21 June 2012 - 11:20 AM

My clay bodies (I use well more than one) are a combination of commercial bodies, altered commercial bodies, and my own blends. I have a batch mixer that I had built for me by a grad student at Mass College of Art (where I worked YEARS ago....like mid 70s) that is like the old Bluebird mixers. Still working.

Since it seems these days that about 90% of people doing claywork use commercial bodies..... I'll constrain my answers to that aspect.

I use Sheffield Pottery Supply as my main supplier. They are in western Massachusetts ...and I am in southern New Hampshire. They have provided great product and service over the years.

From them, I utilize a couple of bodies.

One is their version of the so-called "Z" clay. But I rarely use it unaltered. Usually it has granite dust (from fines up to 1/4" chunks) added to it, as well as often some sand from the river that surrounds my property and occasionally some local red clay.

One of my FAVORITE clay bodies is their "Sheffield #42". This is one that I DO often use unaltered. It contains Lizella, is very dark iron-bearing, and is the closest thing (with one runner-up......see below) I have found in commercial clays available here in America to some iof the clays I use when I am working in Japan. This too often gets granite dust and sand.....but nev er local red clay. It is said to be oxidation only and recommended for cone 8. I fire it in the noborigama up to cone 11 and in reduction for smaller items. It is beautiful. Works well with charcoal youhen (ala' Bizen process).

The other "sort-of-like-Japanese-clay" clay body I use a little of is "Grogzilla" (LOVE the name!) available from Clay Planet on the west coast. No one on the east coast stocks it.... so the shipping costs me more than the clay when I order it. It is a bit similar to some of the Shigaraki/Iga clay. This too often gets the granite dust and sand added....and gets really "nasty" (in a nice way....... wabi-sabi stuff).

My work is a blend of about 50% thrown and 50% handbuilt. About 99.9999999% noborigama woodfired.....but some overglaze enamels in an electric kiln are added.

best,

.......................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#5 User is offline   JBaymore Icon

  • Moderator
  • Icon
  • View gallery
  • Group: Moderators
  • Posts: 1,555
  • Joined: 06-April 10
  • LocationWilton, NH USA

Posted 25 June 2012 - 02:31 PM

WOW.... 4500 views................ and only about four postings!!!!!



Come on folks......... there clearly is an interest in this topic. Share your thoughts....don't just look.



best,


........................john
John Baymore
Immediate Past President; Potters Council
Professor of Ceramics; New Hampshire Insitute of Art

http://www.JohnBaymore.com
0

#6 User is offline   Matt Oz Icon

  • Advanced Procrastinator
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 206
  • Joined: 16-December 11

Posted 28 June 2012 - 06:07 PM

Cone 6 translucent porcelain, because I like messing with light.


0

#7 User is offline   joe.darling Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 26-August 12
  • LocationSydney, Australia

Posted 26 August 2012 - 08:58 PM

Here in Sydney Australia, I most enjoy Keane's "Number 1" earthenware. It's an earthy dark brown medium grog clay with something special. I like it because of the elasticity, body... Spirit maybe within this clay. Throwing this clay is like working in a collabrotive project. The clay boldly moves and sometimes get ahead of me shaping itself before I shape it. It is a pleasure to work with. Try it if you ever come to Sydney!
0

#8 User is offline   Chris Campbell Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,399
  • Joined: 07-April 10
  • LocationRaleigh, NC

Posted 27 August 2012 - 10:10 AM

I use Southern Ice Porcelain because I am totally addicted to it. My work is all colored porcelain and the colors just POP while the white stays incredibly translucent.
For teaching workshops, I use more forgiving friendly Cone 6 porcelains or white clays ... whatever the local supplier has or Highwater Clay's P5 or Little Loafers.

Attached File(s)


Chris Campbell
Contemporary Fine Colored Porcelain
www.ccpottery.com

"My Artwork would not exist without a thriving global pottery community.
In the isolation of a studio, an artist can begin to feel like an island, but in truth
we are all part of archipelagoes; chains of islands loosely connected by a stream
of information that enhances our Artwork.”
1

#9 User is offline   DeLosMares Icon

  • Newbie
  • Pip
  • Group: Members
  • Posts: 1
  • Joined: 26-September 12

Posted 27 September 2012 - 12:25 AM

I have been using Black Mountain from laguna clay for a while now, it has great elasticity, a little slippy on the wheel(but i throw with slip so it works well), and its a really beautiful rich, earthy, dark brown clay. I like it a lot except for how difficult it is to glaze because of how much iron is in the body. I was wondering if anyone knows of a clay that has great elasticity for throwing, and is just as earthy but not as dark as the Black Mountain.
0

#10 User is offline   Edith Marie Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 42
  • Joined: 25-April 12
  • LocationHelena Montana

Posted 27 September 2012 - 06:49 AM

Good Morning everyone,

Haven’t found one clay body I like better than another, so if I had to pick it would be purge. Purge can be light or dark body depending on what has been made and available when I wonder into the Archie Bray Clay Biz where I purchase all my ceramic supplies. Going on a trip, even a golfing trip, with Google at my fingertips I look for Pottery & Supplies for a new adventure into the world of pottery in another state.

Edie



0

#11 User is offline   Cass Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 155
  • Joined: 12-September 12
  • LocationMontana

Posted 27 September 2012 - 07:27 AM

laguna WSO stoneware...for me, the ultimate raku body
0

#12 User is offline   Denice Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 472
  • Joined: 02-April 10
  • LocationWichita, Kansas

Posted 27 September 2012 - 09:06 AM

Only Laguna clay has been sold in this area I have always used it, but the ceramic supply store has started carrying a new line Flinthill Clay. I haven't been able to find very much about it but I'm going to give it a try. Denice
0

#13 User is offline   voceramics Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 34
  • Joined: 28-June 12
  • LocationPaducah, KY

Posted 27 September 2012 - 03:55 PM

Laguna's Hawaiin Red is my all time favorite clay. Just fabulous for hand building and glazes look absolutely amazing on it, deeper and richer. And it loves to keep its form without warping. Since moving eastward we don't have access to that clay, but I still miss it.
Phuong
Vo Studio Ceramics
www.vostudioceramics.etsy.com
0

#14 User is offline   TJR Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 739
  • Joined: 07-December 11
  • LocationCanada

Posted 27 September 2012 - 10:15 PM

I was just at the ceramic supply store yesterday. I picked up 5 boxes of Danish White which is from Laguna. It is a white porcelaineous stoneware. Sometimes I get it with sand if I am making bakers.I also use Plainsman products. They have an open pit clay mine in Medicine Hat Alberta. I use their porcelain P580.
For my high school art classes I use M340 which is a white mid range body that fires to Cone 6. I buy 20 boxes at a time. This amount usually lasts a semester.
Tom[TJR]
0

#15 User is online   Mark C. Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,436
  • Joined: 09-January 12
  • LocationNear Arcata Ca-redwood rain forest

Posted 28 September 2012 - 09:53 PM

Laguna's Dave's porcelain for me for reduction work.
For baking dishes I like half and half from Laguna the smoother one as there are two.
I like various stonewares for salt work-

Mark
Mark Cortright
www.liscomhillpottery.com
0

#16 User is offline   Marcia Selsor Icon

  • Advanced member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 2,505
  • Joined: 16-May 10
  • LocationBrownsville, TX

Posted 29 September 2012 - 03:30 PM

I am liking Limoges Porcelain while I am working in Vallauris, France. It throws beautifully.
Marcia
Marcia Selsor
0

#17 User is online   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,107
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 30 September 2012 - 08:31 AM

View PostMarcia Selsor, on 29 September 2012 - 04:30 PM, said:

I am liking Limoges Porcelain while I am working in Vallauris, France. It throws beautifully.
Marcia


Must be great to work with a famous French porcelain. How translucent is it? I hope you post pics.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#18 User is online   OffCenter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 1,107
  • Joined: 01-April 10
  • LocationLizella, Georgia

Posted 30 September 2012 - 08:35 AM

I like Lizella Red.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.
0

#19 User is offline   Brian Reed Icon

  • Advanced Member
  • PipPipPip
  • Group: Members
  • Posts: 108
  • Joined: 14-August 12
  • LocationWashington State

Posted 02 October 2012 - 12:00 AM

being here in Seattle I have two cone 10 clay bodies that I like to use from Seattle Pottery Supply. One is Kenzan Porcelain and the other is a heavy grog stoneware called Bruning. Both are prepared clays that I buy in bags. They also recycle together nicely with a little Lincoln fire clay added.

I did recently buy some Dakota White Stoneware from Clay Art Center in Tacoma that I am going to try soon.
Brian Reed

Throwing down in Washington State

http://www.reedpottery.com

Northwest Clay Club
0

#20 User is offline   Idaho Potter Icon

  • Advanced Member
  • PipPipPip
  • View gallery
  • Group: Members
  • Posts: 316
  • Joined: 26-August 10
  • LocationBoise, Idaho

Posted 02 October 2012 - 05:18 PM

As most of my work is Raku, my favorite is Coleman Raku from Clay Art Center. White body fires well under extreme circumstances--loss rate is usually very low, less than 10%.

Shirley
0

  • (2 Pages)
  • +
  • 1
  • 2
  • You cannot start a new topic
  • You cannot reply to this topic

1 User(s) are reading this topic
0 members, 1 guests, 0 anonymous users