I hope this question hasnt been asked and answered in the past... If so, I apologize.
I have a Pacifica 800 wheel that is about 10 years old and has always worked perfectly with light to moderate use. Recently when I stop the wheel with the foot pedal the wheel continues to turn slowly... Very annoying. An online search of possible solutions has not helped. Has anyone else experienced this and can you offer suggestions on how to adjust the speed?
Thanks in advance,
Cheryl (aka I love ice cream .... )
#2
Posted 01 June 2012 - 09:50 PM
Iloveicecream, on 01 June 2012 - 06:37 PM, said:
Did you check to see if there was anything built up on, or stuck between, the pedal and base that might be keeping the pedal from totally turning off the power? Sometimes clay slop gets in the pedal joint and needs to be cleaned off.
#3
Posted 02 June 2012 - 06:42 AM
Dharsi, on 01 June 2012 - 09:50 PM, said:
Iloveicecream, on 01 June 2012 - 06:37 PM, said:
Did you check to see if there was anything built up on, or stuck between, the pedal and base that might be keeping the pedal from totally turning off the power? Sometimes clay slop gets in the pedal joint and needs to be cleaned off.
Hi, thanks for your advice. I did clean everything up on the pedal and that did not fix the problem... Any other ideas?
#4
Posted 02 June 2012 - 10:08 AM
Kiln Repair Tech
L&L Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com
neil@neilestrickgallery.com
#5
Posted 02 June 2012 - 12:25 PM
neilestrick, on 02 June 2012 - 10:08 AM, said:
Than you Neil, I'm going to go trouble-shoot now. Will let you know how it goes.
Cheryl
#6
Posted 12 June 2012 - 12:16 PM
Last year replaced the peddle with a new one because mine got wet and corroded inside.
This year after a couple days of throwing the wheel head would not stop turning without switching it on/off several times, finally wouldn't stop at all.
Imagine having a gaggle of pots ready to trim and this happening....
Laguna was quick to repair and return the peddle.
I asked what they did to repair and was told by the service guy Segio:
Quote
So, I doubt you'll be able to repair it yourself.
#7
Posted 12 June 2012 - 03:25 PM
Rapid Dog, on 12 June 2012 - 12:16 PM, said:
Last year replaced the peddle with a new one because mine got wet and corroded inside.
This year after a couple days of throwing the wheel head would not stop turning without switching it on/off several times, finally wouldn't stop at all.
Imagine having a gaggle of pots ready to trim and this happening....
Laguna was quick to repair and return the peddle.
I asked what they did to repair and was told by the service guy Segio:
Quote
So, I doubt you'll be able to repair it yourself.
With the idea it might not be too hard to implement.
What would be needed is a waterproof momentary switch (someone like Graingers would be a place to look)
then it would just need to be placed where the switch would activate either close or open depending on how it's positioned
#8
Posted 13 June 2012 - 10:07 AM
Rapid Dog, on 12 June 2012 - 11:16 AM, said:
Last year replaced the peddle with a new one because mine got wet and corroded inside.
This year after a couple days of throwing the wheel head would not stop turning without switching it on/off several times, finally wouldn't stop at all.
Imagine having a gaggle of pots ready to trim and this happening....
Laguna was quick to repair and return the peddle.
I asked what they did to repair and was told by the service guy Segio:
Quote
So, I doubt you'll be able to repair it yourself.
So they have a design flaw that they are aware of. And rather than correct the problem with a different potentiometer or a redesign of the foot pedal, they just wait for a customer to have a problem and then add another part to compensate. Classic.